Nanoindentation and incipient plasticity

  • E. B. Tadmor (a1), R. Miller (a1), R. Phillips (a1) and M. Ortiz (a2)
Abstract

This paper presents a large-scale atomic resolution simulation of nanoindentation into a thin aluminum film using the recently introduced quasicontinuum method. The purpose of the simulation is to study the initial stages of plastic deformation under the action of an indenter. Two different crystallographic orientations of the film and two different indenter geometries (a rectangular prism and a cylinder) are studied. We obtain both macroscopic load versus indentation depth curves, as well as microscopic quantities, such as the Peierls stress and density of geometrically necessary dislocations beneath the indenter. In addition, we obtain detailed information regarding the atomistic mechanisms responsible for the macroscopic curves. A strong dependence on geometry and orientation is observed. Two different microscopic mechanisms are observed to accommodate the applied loading: (i) nucleation and subsequent propagation into the bulk of edge dislocation dipoles and (ii) deformation twinning.

Copyright
Corresponding author
c)Address all correspondence to this author. e-mail: phillips@engin.brown.edu
Linked references
Hide All

This list contains references from the content that can be linked to their source. For a full set of references and notes please see the PDF or HTML where available.

4.S. J. Sharp , M. F. Ashby , and N. A. Fleck , Acta Metall. Mater. 41, 685 (1993).

5.W.W. Gerberich , J. C. Nelson , E.T. Lilleodden , P. Anderson , and J. T. Wyrobek , Acta Mater. 44, 3585 (1996).

6.N. Gane and F. P. Bowden , J. Appl. Phys. 39, 1432 (1968).

8.P. Tangyunyong , R.C. Thomas , J. E. Houston , T. A. Michalske , R. M. Crooks , and A. J. Howard , Phys. Rev. Lett. 71, 3319 (1993).

10.U. Landman , W. D. Luedtke , N. A. Burnham , and R. J. Colton , Science 248, 454 (1990).

11.J. S. Kallman , W.G. Hoover , C. G. Hoover , A. J. De Groot , S. M. Lee , and F. Wooten , Phys. Rev. B 47, 7705 (1993).

15.E. B. Tadmor , R. Phillips , and M. Ortiz , Langmuir 12, 4529 (1996).

16.V. B. Shenoy , R. Miller , E. B. Tadmor , R. Phillips , and M. Ortiz , Phys. Rev. Lett. 80, 742 (1998).

17.V. B. Shenoy , R. Miller , E. B. Tadmor , D. Rodney , R. Phillips , and M. Ortiz , J. Mech. Phys. Solids 47, 611 (1999).

19.M.S. Daw and M. I. Baskes , Phys. Rev. Lett. 50, 1285 (1983).

20.M.S. Daw , Many-Atom Interactions in Solids, Springer Proceedings in Physics (Springer-Verlag, Berlin, 1990), Vol. 48, p. 48.

21.F. Ercolessi and J. Adams , Europhys. Lett. 26, 583 (1994).

24.A.V. Kulkarni and B. Bhushan , Mater. Lett. 29, 221 (1996).

26.M.J. Mills and P. Stadelmann , Philos. Mag. A 60, 355 (1989).

28.T. Kosugi and T. Kino , Mater. Sci. Eng. A 164, 368 (1993).

29.T. Egami and D. Srolovitz , J. Phys. F: Met. Phys. 12, 2141 (1982).

30.V. Vitek and T. Egami , Phys. Status Solidi B 144, 145 (1987).

35.P. Rosakis and H. Tsai , Mech. Mater. 17, 245 (1994).

37.C.L. Kelchner , S.J. Plimpton , and J.C. Hamilton , Phys. Rev. B 58, 11 085 (1998).

Recommend this journal

Email your librarian or administrator to recommend adding this journal to your organisation's collection.

Journal of Materials Research
  • ISSN: 0884-2914
  • EISSN: 2044-5326
  • URL: /core/journals/journal-of-materials-research
Please enter your name
Please enter a valid email address
Who would you like to send this to? *
×