Influence of Laserglaze on The Microstructure and Wear Resistance Of A Cast Nickel-Base Superalloy

Published online by Cambridge University Press:  21 February 2011

Ge Yunlong
Affiliation:
Institute of Metal Research, Academia Sinica Shenyang, Liaoning, China
Hu Zhuangqi
Affiliation:
Institute of Metal Research, Academia Sinica Shenyang, Liaoning, China
Gao Wei
Affiliation:
Institute of Metal Research, Academia Sinica Shenyang, Liaoning, China
Shih Changhsu
Affiliation:
Institute of Metal Research, Academia Sinica Shenyang, Liaoning, China
Get access

Abstract

Influence of laserglaze on the microstructure and wear resistance of a cast nickel-base superalloy has been studied, which contains very high contents of refractory metals (Mo 33 wt%, W 17 wt%). After surface treatment by laserglaze the alloy structure changes extraordinarily. This change of microstructure enhances the alloy properties. Hardness of the laser melted region is evidently increased, and wear resistance and and corrosion resistance are also improved.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1984

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Breinan, E.M., Physics Today, No. 11, 29 (1976) 44.10.1063/1.3024504Google Scholar
2. Kear, B.H., Breinan, E.M., Greenwald, L.E., Metals Technology, No. 4, 6 (1979) 121.10.1179/030716979803276796Google Scholar
3. Mordike, E.L., Bergmann, H.W., in “Rapidly Solidified Amorphous and Crystalline Alloys” ed. by Kear, B.E., Giessen, B.C., Cohen, M., Boston, MA, USA,(1981) 463.Google Scholar
4. Strutt, P.R., Lewis, B.C., Kear, B.H., in “Rapidly Solidified Amorphous and Crystalline Alloys”, ed. by Kear, B.H., Giessen, B.C., Cohen, M., Boston, MAU SA, (1981) 485.Google Scholar
5. Breinan, E.M., in “Proceedings of the International Conference on Rapid Solidification Processing”, Reston, Virginia, USA (1977) 87.Google Scholar
6. Snow, D.B., in “Superalloy 1980, Proceedings of the Fourth International Symposium of Superalloys), Seven Springs, PA, USA (1980) 189.10.7449/1980/Superalloys_1980_189_203Google Scholar
7. Yun-long, Ge, Jing-yun, Wan, Chang-hsu, Shih, Pract. Met., 19 (1982) 561.Google Scholar
8. Yub-yi, Kuo, Yong-long, Ge, to be published.Google Scholar
9. Mehrabian, R. in ”Solidification Technology” ed. by Burke, J.J., Flemings, M.C., Gorum, A. E., (1971) 300.Google Scholar