Abstract

Nitrogen-doped ZnO (ZnO:N) films have been prepared by remote plasma atomic layer deposition (RP-ALD) and treated by rapid thermal annealing (RTA) in oxygen atmosphere. The local electronic structures of the (ZnO:N) films were investigated by X-ray photoelectron spectroscopy (XPS) and X-ray absorption near edge spectroscopy (XANES) at the O K-edge. The XPS reveals the presence of the Zn-N bond in the ZnO:N films, indicating that partial amounts of oxygen sites are occupied by nitrogen species. This is correspondent with the decrease of electron concentration in ZnO:N films with the nitrogen doping concentration, as indicated by the Hall effect measurement. The RP-ALD technique was applied to fabricate the n-type ZnO:N/p-type GaN heterojunction LEDs. Dominant ultraviolet electroluminescence at 371 nm from the ZnO:N layer was observed at room temperature.

Copyright

Corresponding author

#x002A;E-mail: mjchen@ntu.edu.tw

References

Hide All
1. Huang, M. H., Mao, S., Feick, H., Yan, H. Q., Wu, Y. Y., King, H., Weber, E., Russo, R., and Yang, P., Science 292, 1897 (2001).
2. Rogers, D. J., Hosseini Teherani, F., Yasan, A., Minder, K., Kung, P., and Razeghi, M., Appl. Phys. Lett. 88, 141918 (2006).
3. Guo, X. L., Choi, J. H., Tabata, H. and Kawai, T., Jpn. J. Appl. Phys. Lett. 40, pp. L177L188 (2001).
4. Lim, S. J., Kim, J. M., Kim, D., Kwon, S., Park, J. S., and Kimb, H., J. Electrochem. Soc., 157 (2) H214H218 (2010).
5. Kwon, S., Bang, S., Lee, S., Jeon, S., Jeong, W., Kim, H., Gong, S. C., Chang, H. J., Park, H. H. and Jeon, H., Semicond. Sci. Technol. 24, 035015 (6pp) (2009).
6. Look, D. C., Hemsky, J. W., and Sizelove, J. R., Phys. Rev. Lett. 82, No.12 (1999).
7. Jeong, S. H., Park, B.N., Lee, S. B., Boo, J. H., Thin Solid Films, 516, 55865589 (2008).
8. Wenckstern, H. V., Benndorf, G., Heitsch, S., Sann, J., Brandt, M., Schmidt, H., Lenzner, J., Lorenz, M., kuznetsov, A.Y., Meyer, B. K., Grundmann, M., Appl. Phys. A, 88, 125128 (2007).
9. Ryu, Y. R., Lee, T. S., White, H. W., Appl. Phys. Lett. 83, No.1 (2003).
10. Park, C. H., Zhang, S. B., and Wei, S. H., Phys. Rev. B, 66, 073202 (2002).
11. Liu, W., Gu, S. L., Ye, J. D., Zhu, S. M., Liu, S. M., Zhou, X., Zhang, R., Shi, Y., and Zheng, Y. D., Appl. Phys. Lett. 88, 092101 (2006).
12. Jiao, S. J., Zhang, Z. Z., Lu, Y. M., Shen, D. Z., Yao, B., Zhang, J. Y., Li, B. H., Zhao, D. X., Fan, X. W., and Tang, Z. K., Appl. Phys. Lett. 88, 031911 (2006).
13. Singh, A. V., Mehra, R. M., Wakahara, A. and Yoshida, A., J. Appl. Phys. 93, 396 (2003).
14. Kim, H., Cepler, A., Cetina, C., Knies, D., Osofsky, M.S., Auyeung, R.C.Y., and Piqué, A., Appl Phys A, 93: 593598 (2008).L. L. Chen, J. G. Lu, Z. Z. Ye, Y. M. Lin, B. H. Zhao, Y. M. Ye, J. S. Li, and L. P. Zhu, Appl. Phys. Lett. 87, 252106 (2005).
15. Dunlop, L., Kursumovic, A., MacManus-Driscoll, J. L., Appl. Phys. Lett., 93, 17 (2008).
16. Shih, Y. T., Chien, J. F., Chen, M. J., Yang, J. R., and Shiojiri, M., J. Electrochem. Soc., 158(5) H516H520 (2011).
17. Bencze, K. Z., Kondapalli, K. C. and Stemmler, T. L., Encyclopedia of Inorganic Chemistry, John Wiley & Sons, Ltd. (2008).
18. Joseph, M., Tabata, H., Saeki, H., Ueda, K., Kawai, T., Physica B, 302, 140148 (2001).
19. Jiao, S. J., Zhang, Z. Z., Lu, Y. M., Shen, D. Z., Yao, B., Zhang, J. Y., Li, B. H., Zhao, D. X., and Fan, X. W., Tang, Z. K., Appl. Phys. Lett. 88, 031911 (2006).
20. Chiou, J. W.; Kumar, K. P.; Jan, J. C.; Tsai, H. M.; Bao, C. W.; Pong, W. F.; Chien, F. Z. Auger and Direct Electron Spectra in X-ray Photoelectron Studies of Zinc, Zinc Oxide, Gallium and Gallium Oxide. Appl. Phys. Lett. 85, 3220 (2004).
21. Jirsak, T.; Dvorak, J.; Rodriguez, Jose´ A. Adsorption of NO2 on Rh (111) and Pd/Rh (111): Photoemission Studies. Surf. Sci. 436, L683 (1999).

Related content

Powered by UNSILO

Local Electronic Structure and UV Electroluminescence of n-ZnO:N/p-GaN Heterojunction LEDs Grown by Remote Plasma Atomic Layer Deposition

  • Jui F. Chien (a1), Ching H. Chen (a2), Jing J. Shyue (a1) (a3) and Miin J. Chen (a1) (a4)

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 0 *
Loading metrics...

Abstract views

Total abstract views: 0 *
Loading metrics...

* Views captured on Cambridge Core between <date>. This data will be updated every 24 hours.

Usage data cannot currently be displayed.