Pulsed Laser Deposition of Cluster-Assembled Thin Films with Controlled Nanostructure

Published online by Cambridge University Press:  26 February 2011

Andrea Li Bassi
Affiliation:
andrea.libassi@polimi.it, Politecnico di Milano, Dipartimento di Ingegneria Nucleare, via Ponzio 34/3, Milano, N/A, 20133, Italy, +39 02 2399 6316, +39 02 2399 6309
Carlo Spartaco Casari
Affiliation:
carlo.casari@polimi.it, Italy
Fabio Di Fonzo
Affiliation:
fabio.difonzo@polimi.it, Italy
Alessandro Bailini
Affiliation:
alessandro.bailini@polimi.it, Italy
Matteo Fusi
Affiliation:
matteofusi@virgilio.it, Italy
David Dellasega
Affiliation:
david.dellasega@polimi.it, Italy
Valeria Russo
Affiliation:
valeria.russo@polimi.it, Italy
Andrea Baserga
Affiliation:
andrea.baserga@polimi.it, Italy
Diego Cattaneo
Affiliation:
diego.cattaneo@polimi.it, Italy
Carlo Enrico Bottani
Affiliation:
carlo.bottani@polimi.it, Italy
Get access

Abstract

Thin films synthesized by assembling clusters present interesting chemical and physical properties and a large specific surface, and are appealing for functional applications (e.g. sensing and catalysis). Also, clusters supported on surfaces are interesting both for nanocatalysis applications and for fundamental research. By means of pulsed laser deposition (PLD) in a background atmosphere we can induce cluster aggregation in the ablation plume and control the deposition kinetic energy of the clusters. These phenomena depend on the plume expansion dynamics and their influence on the properties of the deposited films has been investigated as a function of the background gas mass and pressure. The control of these parameters permits variation of the film surface morphology, from a compact structure with a very smooth surface, to a film with a controlled roughness at the nanoscale, to an open, low density meso- and nanostructure characterized by a high fraction of voids and by a large specific area. Thin films of WOx, TiOx, Pd/PdO, and Ag were deposited and characterized by atomic force microscopy (AFM), scanning electron microscopy (SEM) and Raman spectroscopy. Post-deposition annealing permits control of the crystalline degree of the films, which in the case of tungsten and titanium oxide is found to depend on the original nanostructure, while a different degree of oxidation can be induced by controlling the amount of oxygen in the deposition chamber. In-situ scanning tunneling microscopy (STM) was employed to study the first stages of growth of W films on different substrates. This opens the possibility to tailor the material properties through the control of the building nano-units.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Jensen, P., Rev. Mod. Phys. 71, 1695 (1999)Google Scholar
[2] Geohegan, D.B., Puretzky, A.A., Duscher, G., and Pennycook, S.J., Appl. Phys. Lett. 72, 2987 (1998)Google Scholar
[3] Dolbec, R., Irissou, E., Chaker, M., Guay, D., Rosei, F., and Khakhani, M.A. El, Phys. Rev. B 70, 201406 (2004)Google Scholar
[4] Lowndes, D.H., Rouleau, C.M., Thundat, T.G., Duscher, G., Kenik, E.A., Pennycook, S.J., J. Mater. Res. 14, 359 (1999)Google Scholar
[5] Chrisey, D. B. and Hubler, G., “Pulsed Laser Deposition of Thin Films”, Wiley & Sons, New York (1994)Google Scholar
[6] Willmott, P.R. and Huber, J.R., Rev. Mod. Phys. 72, 315 (2000)Google Scholar
[7] Kawasaki, H., Namba, J., Iwatsuji, K., Suda, Y., Wada, K., Ebihara, K., and Ohshima, T., Appl. Surf. Sci. 197–198, 547 (2002)Google Scholar
[8] Salje, E. and Viswanathan, K., Acta Cryst. A 31, 356 (1975)Google Scholar
[9] Fujishima, A., Rao, T. N., and Tryk, D. A., J. Photochem. Photobiol. C 1, 1 (2000)Google Scholar
[10] Gratzel, M., Nature 414, 338 (2001)Google Scholar
[11] Amoruso, S., Bruzzese, R., Spinelli, N., Velotta, R., Vitiello, M., and Wang, X., Phys. Rev. B 67, 224503 (2003)Google Scholar
[12] Budtz-Jørgensen, C.V., Mond, M.M., Doggett, B., and Lunney, J.G., J. Phys. D: Appl. Phys. 38, 1892 (2005)Google Scholar
[13] Chen, X.Y., Xiong, S.B., Sha, Z.S. and Liu, Z.G., Appl. Surf. Sci. 115, 279 (1997)Google Scholar
[14] Boulova, M. and Lucazeau, G., Journal of Solid State Chemistry 167, 423 (2002)Google Scholar
[15] Boulova, M., Gaskov, A, and Lucazeau, G., Sens. and Act. B 81, 99 (2001)Google Scholar
[16] Bassi, A. Li, Cattaneo, D., Russo, V., Bottani, C.E., Barborini, E., Mazza, T., Piseri, P., Milani, P., Ernst, F.O., Wegner, K., and Pratsinis, S.E., J. Appl. Phys. 98, 074305 (2005)Google Scholar