Structural Analyses and Magnetic Properties of Multiple-Structure Multilayered Co/Au Films

Published online by Cambridge University Press:  01 February 2011

Rimika Koiwai
Affiliation:
Department of Material Science, Chiba Institute of Technology, 2-17-1 Narashino-shi, Tsudanuma, Chiba 275-0016, Japan Advanced Device Laboratory, Oki Electric Industry Co. Ltd., 550-5 Higashiasakawa, Hachioji-shi, Tokyo 193-8550, Japan
Masanobu Kobayashi
Affiliation:
Department of Material Science, Chiba Institute of Technology, 2-17-1 Narashino-shi, Tsudanuma, Chiba 275-0016, Japan Advanced Device Laboratory, Oki Electric Industry Co. Ltd., 550-5 Higashiasakawa, Hachioji-shi, Tokyo 193-8550, Japan
Yoshinori Maeno
Affiliation:
Department of Material Science, Chiba Institute of Technology, 2-17-1 Narashino-shi, Tsudanuma, Chiba 275-0016, Japan Advanced Device Laboratory, Oki Electric Industry Co. Ltd., 550-5 Higashiasakawa, Hachioji-shi, Tokyo 193-8550, Japan
Get access

Abstract

In the interfaces of multilayered Co/Au and Co/Pd films, there were some interesting changes with annealing. For profile fittings, which is a comparison between measured peaks of X-ray diffraction and calculated peaks of the extended 3-step model profile fittings, the mixed layers between Co layers and noble metal layers were decreased in Co/Au films while increased in Co/Pd films. These results are based on the difference that Co-Au is a eutectic system while Co-Pd is an isomorphous system. This time, as new research, we fabricated multiple-structure multilayered Co/Au films (MSM Co/Au films). Magnetic properties and structural analyses were carried out with a vibrating sample magnetometer (VSM), X-ray diffraction (XRD), and extended 3-step model profile fittings. MSM Co/Au films have two periodic thicknesses. MSM Co/Au films showed the same perpendicular magnetization as Co/Au and Co/Pd films, which is dependent on the Co layer thickness. Perpendicular magnetization showed the maximum value after 1 h-annealing at 473 K. It was well confirmed that the mixed layers decreased at this annealing condition with the extended 3-step model profile fittings.

Type
Research Article
Copyright
Copyright © Materials Research Society 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Fujimori, H., in Artificial Metallic Superlattices, edited by Nagasaki, S. (Agne Technical Center, Japan, 1995), pp. 1928.Google Scholar
2. Maeno, Y., Yamane, H., Sato, K., and Kobayashi, M., Appl. Phys. Lett. 60 (4), 510511 (1992).Google Scholar
3. Koiwai, R., Koduka, Y., Ishii, T., Maeno, Y., and Kobayashi, M., Trans. Mater. Res. 26 (4), 12751278 (2001).Google Scholar
4. Underwood, J. H. and Barbee, T. W. Jr, Appl. Opt. 20 (17), 30273034 (1981).Google Scholar