Ta/low-κ CMP with Colloidal Silica Particles

Published online by Cambridge University Press:  01 February 2011

Patrice Beaud
Affiliation:
Swiss Federal Institute of Technology, Electronics Laboratory, CH-1015 Lausanne, Switzerland
Didier Bouvet
Affiliation:
Swiss Federal Institute of Technology, Electronics Laboratory, CH-1015 Lausanne, Switzerland
Pierre Fazan
Affiliation:
Swiss Federal Institute of Technology, Electronics Laboratory, CH-1015 Lausanne, Switzerland
Eric Jacquinot
Affiliation:
Life Science & Electronic Chemicals Division, Clariant (France), BP1, 60350 Trosly Breuil, France
Hiroyuki Aoki
Affiliation:
Polysilazane Business Group, Life Science and Electronic Chemicals Division, Clariant (JAPAN) K.K.
Tomoko Aoki
Affiliation:
Polysilazane Business Group, Life Science and Electronic Chemicals Division, Clariant (JAPAN) K.K.
Get access

Abstract

Low-κ/Cu interconnect integration achievement is one of the key issues for the future sub-100 nm technologies. Nowadays, no definitive integration scheme has been reported. Low-κ integration is especially difficult because the trench/via etching and CMP processes can damage its properties. In the present work, we present results on different materials that could be used in such integration. We focused our study on the barrier (Ta/TaN) and on a low-κ material (dense and porous), that is a spin-on-dielectric (SOD) of the methylsilsesquioxane (MSQ) type. CMP slurries were made from monodisperse colloidal silica particles. In a first approach, the slurries compositions mainly differed by their pH and abrasive characteristics. The particle size ranged from 12 to 80 nm, with a pH varying between 2 and 11. The sensitivity of the Ta/TaN and low-κ removal rates will also be reported. Scanning electron microscopy (SEM) and atomic force microscopy (AFM) of the different films were carried out in order to evaluate the impact of CMP on their surface quality. Measurements did not show any surface degradation or/and scratches, and no delamination has been observed. Post-CMP κ value measurements have been carried out to highlight possible damage on the low-ê dielectric materials.

Type
Research Article
Copyright
Copyright © Materials Research Society 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Iler, R. K., The Chemistry of silica: solubility, polymerization, colloid and surface properties, and biochemistry. New York: John Wiley & Sons, Inc., 1979.Google Scholar
[2] Sears, G. W., “Determination of Specific Surface Area of Colloidal Silica by Titration with Sodium Hydroxide,” Analytical Chemistry, vol. 28, pp. 19811983, 1956.Google Scholar
[3] Steigerwald, Joseph M., Murarka, Shyam P., and Gutmann, R. J., Chemical Mechanical Planarization of Microelectronic Materials. New York: John Wiley Sons, Inc., 1997.Google Scholar
[4] Kim, H. G., An, Y. M., Moon, D. K., and Park, J. G., “Effect of chemicals and slurry particles on chemical mechamical polishing of polyimide,” Japanese Journal of Applied Physics Part 1-Regular Papers Short Notes & Review Papers, vol. 39, pp. 10851090, 2000.Google Scholar
[5] Hariharaputhiran, M., Li, Y., Ramarajan, S., and Babu, S. V., “Chemical mechanical polishing of Ta,” Electrochemical and Solid State Letters, vol. 3, pp. 9598, 2000.Google Scholar