Hostname: page-component-76fb5796d-dfsvx Total loading time: 0 Render date: 2024-04-25T10:16:42.544Z Has data issue: false hasContentIssue false

Integration Issues of (Ba,Sr)TiO3Thin Films in High Density Devices

Published online by Cambridge University Press:  10 February 2011

C. Y. Yoo
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
H. B. Park
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
D. S. Hwang
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
H. Hideki
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
W. D. Kim
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
H. J. Lim
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
B. T. Lee
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
Y. W. Park
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
S. I. Lee
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
M. Y. Lee
Affiliation:
Process Development Team, Semiconductor R&D Center, Samsung Electronics Co., Ltd., San #24, Nongseo-Ree, Kiheung-Eup, Yongin-Si, Kyungki-Do, 449–900, Korea (ROK)Tel#82–331–209–6324, #82–33 1–209–6299, yoocyq@samsung.co.kr
Get access

Abstract

Recent progress to overcome integration issues related with (Ba,Sr)TiO3 films are presented. Firstly, ternary barrier material, Ti0.7Al0.3N deposited by reactive sputtering is shown to have superior oxidation resistance than TiN through the test using contact string pattern where Pt is deposited as a electrode. Ti0.7Al0.3N barrier is able to keep stable contact resistance below 100Ω even under oxidizing condition where the temperature is 550°C and oxygen partial pressure is 7.6 Torr. If rapid thermal annealing is used, annealing temperature without oxidation of Ti0.7Al0.3N can be increased by about 100°C. Ti0.7Al0.3N is thought to be the promising one which can endure during post-annealing process. Secondly, electroplating technology is employed to fabricate the stack capacitor of Pt that has been known to be very difficult to etch. 500Å-thick Pt is used as a seed layer and very thick Pt is selectively grown on the seed layer by the electroplating. The Pt height can be controlled by changing the electroplating time, so we can make stack Pt over 8000Å. Thirdly, low temperature deposition process for MOCVD BST film is developed. The equivalent oxide thickness of about 3.5Å is obtained on Pt electrode when BST thickness is 150Å. BST film is deposited at 420°C and annealed at 700°C under oxidizing atmosphere. It is suggested that a new two step annealing consisting of high temperature annealing under inert atmosphere and low temperature annealing under oxidizing atmosphere is very effective to achieve the high dielectric constant and low leakage current of BST films at the same time. It is also adequate for preventing the barrier oxidation. BST film with Toxeq. of 5.2Å and low leakage current is obtained by annealing at 650°C under N2 followed by annealing at 550TC under O2. Electrical properties of BST deposited on side-wall of Pt concave capacitor is evaluated. The concave capacitor with about aspect ratio 3 shows the same capacitance and leakage current as the planar capacitor, which implies that BST composition and thickness is uniform on the side-wall. It is concluded that BST films on Pt electrode can be applied to real device.

Type
Research Article
Copyright
Copyright © Materials Research Society 2000

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Kim, K. N., Kwak, D. H., Hwang, Y. S., Jeong, G. T., Chung, T. Y., Park, B. J., Chun, Y. S., Oh, J. H., Yoo, C. Y., Joo, B. S., Symposium on VLSI Technology Digest of Technical Papers, 33 (1999).Google Scholar
2. Hieda, K., Eguchi, K., Nakahira, J., Kiyotoshi, M., Nakabayashi, M., Tomita, H., Izuha, M., Aoyama, T., Niwa, S., Tsunoda, K., Yamazaki, S., Lin, J., Shimada, A., Nakamura, K., Kubota, T., Asano, M., Hosaka, K., Fukuzumi, Y., Ishibashi, Y. and Kohyama, Y., Proceedings of the International Electron Devices Meeting, to be published (1999)Google Scholar
3. Lee, B. T., Lee, K. H., Whang, C. S., Kim, W. D., Horii, H., Kim, H. W., Cho, H. J., Kang, S. S., Lee, S. I., and Lee, M. Y., Proceedings of the International Electron Devices Meeting, 249 (1997)Google Scholar
4. Khamankar, R. B., Kressley, M. A., Visokay, M. R., Moise, T., Xing, G., Nemuto, S., Okuno, Y., Fang, S. J., Wilson, A. M., Gaynor, J. F., Hurd, T. Q., Crenshaw, D. L., Summerfelt, S. and Colombo, L., Proceedings of the International Electron Devices Meeting, 245 (1997)Google Scholar
5. Plokela, P. J., Reid, J. S., Kwok, C. K., Kolawa, E. and Nicolet, M. A., J. Appl. Phys. 70, 2828 (1991)Google Scholar
6. McIntyre, D. and Greene, J. E., J. Appl. Phys. 67, 1542 (1990)Google Scholar
7. Yoon, D. S. and Baik, H. K. and Lee, S. M., Lee, S. I., Ryu, H. and Lee, H. J., J. Vac. Sci. Technol. B 16, 1137 (1998)Google Scholar
8. McIntyre, P. C. and Summerfelt, S., Appl. Phys. Lett. 70, 711 (1997)Google Scholar
9. Hieda, K., Eguchi, K., Fukushima, N., Aoyama, T., Natori, N., Kiyotoshi, M., Yamazaki, S., Izuha, M., Niwa, S., Fukuzumi, Y., Ishibashi, Y., Kohyama, Y., Arikado, T. and Okumura, K., Proceedings of the International Electron Devices Meeting, 807 (1998)Google Scholar
10. Kiyotoshi, K., Yamazaki, S., Eguchi, K., Hieda, K., Fukuzumi, Y., Izuha, M., Aoyama, T., Niwa, S., Nakamura, K., Kojima, A., Tomita, H., Kubota, T., Satoh, M., Kohyama, Y., Tsunashima, Y., Arikado, T. and Okumura, K., Symposium on VLSI Technology Digest of Technical Papers, 101 (1999)Google Scholar
11. Shibano, T., Nakamura, K. and Oomori, T., J Vac.Sci. Technol. A 16, 502 (1998)Google Scholar
12. Athavale, S. D., Gutsche, M., Kotecki, D. E. and Shen, H., Proceedings of the International Electron Devices Meeting to be submitted (1999)Google Scholar
13. Lee, B. T., Yoo, C. Y., Lim, H. J., Kang, C. S., Park, H. B., Kim, W. D., Ju, S. H., Horii, H., Lee, K. H., Kim, H. W., Lee, S. I. and Lee, M. Y., Proceedings of the International Electron Devices Meeting, 815 (1998)Google Scholar
14. Horii, H., Lee, B. T., Lim, H. J., Joo, S. H., Kang, C. S., Yoo, C. Y., Park, H. B., Kim, W. D., Lee, S. I., Lee, M. Y., Symposium on VLSI Technology Digest of Technical Papers, 103 (1999)Google Scholar
15. Kang, C. S., Cho, H. J., Whang, C. S., Lee, B. T., Lee, K. H., Horii, H., Kim, W. D., Lee, S. I., Lee, M. Y., Jpn. J. Appl. Phys. 36, 6946 (1997)Google Scholar
16. Yamamuka, M., Kawahara, T., Makita, T., Yuuki, A., and Ono, L., Jpn. J. Appl. Phys. 35, 729 (1996)Google Scholar
17. Kawahara, T., Yamamuka, M., Yuuki, A. and Ono, K., Jpn. J Appl. Phys. 35, 4880 (1996)Google Scholar
18. Vendik, O. G., Zubko, S. P. and Ter-Martirosayn, L. T., Appl. Phys. Lett. 73, 37 (1998)Google Scholar
19. Natori, K., Otani, D. and Sano, N., Appl. Phys. Lett. 73, 632 (1998)Google Scholar
20. Hwang, C. S., Lee, B. T., Kang, C. S., Kim, J. W., Lee, K. H., Cho, J. J., Hideki, H., Kim, W. D., Lee, S. I., Koh, Y. B. and Lee, M. Y., J. Appl. Phys. 83, 3703 (1998)Google Scholar
21. Maruno, S., Kuroiwa, T., Mikami, N. and Sato, K., Appl. Phys. Lett. 73, 954 (1998)Google Scholar
22. Yamamuka, M., Kawahara, T., Makita, T., Yuuki, A., and Ono, K., Jpn. J Appl. Phys. 35, 2530 (1996)Google Scholar