Characterization of White and Black Deposits on the Surface of Korean Stone Cultural Heritages

Published online by Cambridge University Press:  06 August 2013

Jiyoung Kim
Affiliation:
Department of Cultural Heritage Conservation Sciences, Kongju National University, Shinkwan-dong 182, Gongju, Chungnam Province 314-701, Republic of Korea
Chan Hee Lee*
Affiliation:
Department of Cultural Heritage Conservation Sciences, Kongju National University, Shinkwan-dong 182, Gongju, Chungnam Province 314-701, Republic of Korea
Ran Hee Kim
Affiliation:
Department of Cultural Heritage Conservation Sciences, Kongju National University, Shinkwan-dong 182, Gongju, Chungnam Province 314-701, Republic of Korea
Eun Jeong Shin
Affiliation:
Conservation Science Division, National Research Institute of Cultural Heritage, Daejeon 305-380, Republic of Korea
*
*Corresponding author. E-mail: chanlee@kongju.ac.kr
Get access

Abstract

White and black deposits have been frequently observed on the surface of Korean stone cultural heritages, and they are considered as damage factors in both conservation and esthetic points of view. In order to set up the appropriate conservation remedy, it is important to know their origins, characteristics, and compositions. In this study, optical and scanning electron microscopes (SEMs) equipped with an energy-dispersive spectrometer (EDS) and X-ray diffractometer were employed to determine the white and black deposits. It was found that both deposits consisted mainly of calcium carbonate (calcite) and calcium sulfate (gypsum). The calcite and gypsum were characterized by bladed, rhombohedral, tabular, and amorphous morphologies under a SEM. The black deposit was not only composed of calcite or gypsum, but also accompanied amorphous and irregular matrix. SEM-EDS analysis revealed an abundance of silicon, aluminum, iron, phosphorus, and carbon on the matrix, which were major elements of soil, atmospheric deposits, and organisms. The white deposit, on the other hand, barely contained those coloring substances. These salts and deposited substances were caused by chemical reaction and physical adhesion between rock-forming minerals, lime mortar, sulfur in polluted air environment, soil dust, and microorganisms.

Type
Research Article
Copyright
Copyright © Microscopy Society of America 2013 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Bugini, R., Tabasso, M.L. & Realini, M. (2000). Rate of formation of black crusts on marble. J Cult Herit 1, 111116.Google Scholar
Camuffo, D. (1981). Hot horse anemometry. Atmos Environ 15, 1767.Google Scholar
Camuffo, D. (1995). Physical weathering of stones. Sci Total Environ 167, 114.Google Scholar
Charola, A.E., Pühringer, J. & Steiger, M. (2007). Gypsum: A review of its role in the deterioration of building materials. Environ Geol 52, 339352.Google Scholar
Chesworth, W. (1971). The major element geochemistry and the mineralogical evolution of granitic rocks during weathering. In Origin and Distribution of Elements, Ahrens, L.H. (Eds.), pp. 305313. Oxford, UK: Pergamon Press.Google Scholar
Gaylarde, C.C., Ortega-Morales, B.O. & Bartolo-Pérez, P. (2007). Biogenic black crusts on buildings in unpolluted environment. Curr Microbiol 54, 162166.Google Scholar
Grossi, C.N., Esbert, R.M., Diaz-Pache, F. & Alonso, F.J. (2003). Soiling of building stones in urban environments. Build Environ 38, 147159.Google Scholar
Guido, C.G., Paola, B., Darinn, C., Guiseppe, C. & Rocco, M. (1997). Chemical characterization of the black crust present on the stone central portal of St. Denis abbey. Anal Bioanal Chem 357, 12111214.Google Scholar
Lee, C.H., Choi, S.W. & Suh, M. (2003). Natural deterioration and conservation treatment for the granite standing Buddha of Daejosa Temple, Republic of Korea. Geotech Geol Eng 21, 6377.Google Scholar
Lee, C.H., Lee, M.S., Suh, M. & Choi, S.W. (2005). Weathering and deterioration of rock properties of the Dabotap pagoda (World Cultural Heritage), Republic of Korea. Environ Geol 47, 547557.Google Scholar
Lee, D.S., Lee, C.H., Kim, J. & Yang, H.J. (2008). Geochemical characteristics of surface efflorescence on the seventh century stone pagoda in Republic of Korea. Environ Geol 58, 197204.Google Scholar
Maravelaki-Kalaitzaki, P. (2005). Black crusts and patinas on Pentelic marble from the Parthenon and Erechtheum (Acropolis, Athens): Characterization and origin. Anal Chim Acta 532, 187198.Google Scholar
Moropoulou, A., Bisbikou, K., Torfs, K., Van Grieken, R., Zezza, F. & Marci, F. (1998). Origin and growth of weathering crusts on ancient marbles in industrial atmosphere. Atmos Environ 32, 967982.Google Scholar
Sabbioni, C. (1995). Contribution of atmospheric deposition to the formation of damage layers. Sci Total Environ 167, 4955.Google Scholar
Török, A. (2008). Black crusts on travertine: Factors controlling development and stability. Environ Geol 56, 583594.Google Scholar
Warscheid, T. & Braams, J. (2000). Biodeterioration of stone: A review. Int Biodeter Biodegr 46, 343368.Google Scholar
Winkler, E.M. (1987). Weathering and weathering rates of natural stone. Environ Geol 9, 8592.Google Scholar
Wright, J.S. (2002). Geomorphology and stone conservation: Sandstone decay in Stoke-on-Trent. Struct Surv 20, 5061.Google Scholar