Hostname: page-component-848d4c4894-p2v8j Total loading time: 0.001 Render date: 2024-06-05T01:44:03.257Z Has data issue: false hasContentIssue false

Direct Contacting with Liquid Electrolyte Facilitates the Surface Phase Transition in Ni-rich Layered Cathode

Published online by Cambridge University Press:  30 July 2020

Lianfeng Zou
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Wengao Zhao
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Haiping Jia
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Jianming Zheng
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Linze Li
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Daniel Abraham
Affiliation:
ANL, Lemont, Illinois, United States
Guoying Chen
Affiliation:
LBNL, Berkeley, California, United States
Jason Croy
Affiliation:
ANL, Lemont, Illinois, United States
Ji-Guang Zhang
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States
Chongmin Wang
Affiliation:
Pacific Northwest National Laboratory, Richland, Washington, United States

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Energy and Soft Materials and the Development of Cryogenic Techniques for Studying Them
Copyright
Copyright © Microscopy Society of America 2020

References

Betz, J.; Brinkmann, J. P.; Nölle, R.; Lürenbaum, C.; Kolek, M.; Stan, M. C.; Winter, M.; Placke, T. Cross Talk between Transition Metal Cathode and Li Metal Anode: Unraveling Its Influence on the Deposition/Dissolution Behavior and Morphology of Lithium. Adv. Energy Mater. 2019, 9, 1900574.10.1002/aenm.201900574CrossRefGoogle Scholar
Gilbert, J. A.; Shkrob, I. A.; Abraham, D. P. Transition metal dissolution, ion migration, electrocatalytic reduction and capacity loss in lithium-ion full cells. J. Electrochem. Soc. 2017 , 164, A389-A399.10.1149/2.1111702jesCrossRefGoogle Scholar
Li, W.; Kim, U.-H.; Dolocan, A.; Sun, Y.-K.; Manthiram, A. Formation and inhibition of metallic lithium microstructures in lithium batteries driven by chemical crossover. ACS nano 2017 , 11, 5853-5863.10.1021/acsnano.7b01494CrossRefGoogle ScholarPubMed
Zheng, H.; Sun, Q.; Liu, G.; Song, X.; Battaglia, V. S. Correlation between dissolution behavior and electrochemical cycling performance for LiNi1/3Co1/3Mn1/3O2-based cells. J. Power Sources 2012 , 207, 134-140.10.1016/j.jpowsour.2012.01.122CrossRefGoogle Scholar
Zou, L.; Li, J.; Liu, Z.; Wang, G.; Manthiram, A.; Wang, C. Lattice doping regulated interfacial reactions in cathode for enhanced cycling stability. Nat. Commun. 2019 , 10, 3447.10.1038/s41467-019-11299-2CrossRefGoogle ScholarPubMed
Lin, F.; Markus, I. M.; Nordlund, D.; Weng, T.-C.; Asta, M. D.; Xin, H. L.; Doeff, M. M. Surface reconstruction and chemical evolution of stoichiometric layered cathode materials for lithium-ion batteries. Nat. Commun. 2014 , 5, 3529.10.1038/ncomms4529CrossRefGoogle ScholarPubMed
Maleki Kheimeh Sari, H.; Li, X. Controllable Cathode–Electrolyte Interface of Li [Ni0. 8Co0. 1Mn0. 1] O2 for Lithium Ion Batteries: A Review. Adv. Energy Mater. 2019 , 9, 1901597.10.1002/aenm.201901597CrossRefGoogle Scholar
Li, T.; Yuan, X.-Z.; Zhang, L.; Song, D.; Shi, K.; Bock, C. Degradation mechanisms and mitigation strategies of nickel-rich NMC-based lithium-ion batteries. Electrochem. Energy Rev. 2019, 1-38.Google Scholar
Lin, F.; Nordlund, D.; Li, Y.; Quan, M. K.; Cheng, L.; Weng, T.-C.; Liu, Y.; Xin, H. L.; Doeff, M. M. Metal segregation in hierarchically structured cathode materials for high-energy lithium batteries. Nat. Energy 2016 , 1, 15004.10.1038/nenergy.2015.4CrossRefGoogle Scholar