TEM Study of Growth Defects in CVD Diamond Films

Published online by Cambridge University Press:  15 February 2011

Fred Y. Chen
Affiliation:
Department of Materials Science & Engineering, State University of New York at Stony Brook, Stony Brook, NY 11794–2275
Alexander H. King
Affiliation:
Vactronic Lab. Equipment, Inc., 160 Wilbur Place, Bohemia, NY 11716
Robert F. Salat
Affiliation:
Vactronic Lab. Equipment, Inc., 160 Wilbur Place, Bohemia, NY 11716
Glenn J. Fricano
Affiliation:
Vactronic Lab. Equipment, Inc., 160 Wilbur Place, Bohemia, NY 11716
Get access

Abstract

Transmission electron microscopy (TEM) has been used to examine defects in diamond films grown by the microwave plasma-enhanced chemical vapor deposition (CVD) method. Graphite was used as the sole carbon source during the CVD process with silicon substrates. Growth defects including twins, stacking faults, dislocations and second-phase precipitates were observed in the films. In plan-view TEM, defect clusters at the centers of diamond grains were observed, where the film is also the thickest. Cross-sectional TEM was carried out to show that the defect clusters fan out from a single nucleation site in each grain, at the diamond-silicon interface. Possible growth mechanisms of the defect clusters in diamond grains are considered.

Type
Research Article
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Kawarada, H., Mar, K.S., Suzuki, J., Ito, T., Mori, H., Fujita, H. and Hiraki, A., Jpn. J. Appl. Phys. 26, L1903 (1987)Google Scholar
2. Williams, B.E. and Glass, J.T., J. Mater. Res., 4, 373 (1989)Google Scholar
3. Clausing, R.E., Heatherly, L., More, K.L., and Begun, G.M., Surface and Coatings Technology, 39/40, 199 (1989)Google Scholar
4. Kaae, J.L., Gantzel, P.K., Chin, J., and West, W.P., J. Mater. Res. 5, 1480 (1990)Google Scholar
5. Luyten, W., Van Tendeloo, G., Amelinckx, S., and Collins, J.L., Phil. Mag. A, 66, 899 (1992)Google Scholar
6. Shechtman, D., Hutchison, J.L., Robins, L.H., Farabaugh, E.N., and Feldman, A., J. Mater. Res., 8, 473 (1993)Google Scholar
7. Chen, F.Y., Bourdillon, A.J., Tan, N., Jeng, D.G., Salat, R.F., and Fricano, G.J., 4th Annual Diamond Technology Workshop, Madison, Wisconsin, March 2426 (1993)Google Scholar
8. Jeng, D.G., Seibles, L., Mitchell, J.W., Chen, F.Y., Bourdillon, A.J., Salat, R.F., and Fricano, G.J., 4th Annual Diamond Technology Workshop, Madison, Wisconsin, March 2426 (1993)Google Scholar
9. Jeng, D.G., Tuan, H.S., Salat, R.F., and Fricano, G.J., Appl. Phys. Lett. 67, 1968 (1990)Google Scholar
10. Zhang, H., J. Thermal Spray Technology, 1, 83 (1992)Google Scholar
11. Edington, J.W., Interpretation of Transmission Electron Micrographs, Volume 3 (1975)Google Scholar
12. Zalm, P.C., Bulle-Lieuwma, C.W.T. and Marée, P.M., Phillips Tech. Rev. 43, 154 (1987)Google Scholar
13. Nandedkar, A.S. and Narayan, J., Phil. Mag. A, 56, 625 (1987)Google Scholar