Summary

Nickel is the fifth most abundant element on earth. The atomic number is 28, and this places it in the first row of the d block of transition metals, alongside iron and cobalt. The atomic weight is 58.71, the weighted average of the five stable isotopes 58, 60, 61, 62 and 64, which are found with probabilities 67.7%, 26.2%, 1.25%, 3.66% and 1.16%, respectively. The crystal structure is face-centred cubic (FCC; see Figure 2.1), from ambient conditions to the melting point, 1455 °C, which represents an absolute limit for the temperature capability of the nickel-based superalloys. The density under ambient conditions is 8907 kg/m3. Thus, compared with other metals used for aerospace applications, for example, Ti (4508 kg/m3) and Al (2698 kg/m3), Ni is rather dense. This is a consequence of a small interatomic distance, arising from the strong cohesion provided by the outer d electrons – a characteristic of the transition metals.

In this chapter, some important aspects of the physical metallurgy of nickel and its alloys are considered. Section 2.1 is concerned with the compositions of the superalloys and the phases promoted by the presence of the alloying elements. Such composition– microstructure relationships have been established over many years, and considerable use of them is required when designing new grades of superalloy.

Information

Type
Chapter
Information
The Superalloys
Fundamentals and Applications
, pp. 33 - 120
Publisher: Cambridge University Press
Print publication year: 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Accessibility standard: Unknown

Accessibility compliance for the PDF of this book is currently unknown and may be updated in the future.

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

Available formats
×