Extraction Replication of Carbides and Borides in the Ni-base Superalloy IN100
Published online by Cambridge University Press: 01 August 2004
Extract
Extended abstract of a paper presented at Microscopy and Microanalysis 2004 in Savannah, Georgia, USA, August 1–5, 2004.