Correlated Post-mortem Raman and TEM Investigation of Nanoindentation Induced Structural Changes in Silicon as a Function of Temperature

Published online by Cambridge University Press:  30 July 2020

Praveena Manimunda
Affiliation:
Bruker Nano Surfaces, Eden Prairie, Minnesota, United States
Eric Hintsala
Affiliation:
Bruker Nano Surfaces, Eden Prairie, Minnesota, United States
Douglas Stauffer
Affiliation:
Bruker Nano Surfaces, Eden Prairie, Minnesota, United States
S.A.S. Asif
Affiliation:
Industron, Thiruvananthapuram, Kerala, India

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Surface and Subsurface Microscopy and Microanalysis of Physical and Biological Specimens
Copyright
Copyright © Microscopy Society of America 2020

References

Weinstein, B. A., & Piermarini, G. J. (1975). Raman scattering and phonon dispersion in Si and GaP at very high pressure. Physical Review B, 12(4), 1172.10.1103/PhysRevB.12.1172CrossRefGoogle Scholar
Minomura, S., & Drickamer, H. G. (1962). Pressure induced phase transitions in silicon, germanium and some III–V compounds. Journal of Physics and Chemistry of Solids, 23(5), 451456.10.1016/0022-3697(62)90085-9CrossRefGoogle Scholar
Jamieson, J. C. (1963). Crystal structures at high pressures of metallic modifications of silicon and germanium. Science, 139(3556), 762764.10.1126/science.139.3556.762CrossRefGoogle ScholarPubMed
Gerbig, Y. B., Michaels, C. A., Forster, A. M., & Cook, R. F. (2012). In situ observation of the indentation-induced phase transformation of silicon thin films. Physical Review B, 85(10), 104102.10.1103/PhysRevB.85.104102CrossRefGoogle Scholar
Domnich, V., Aratyn, Y., Kriven, W. M., & Gogotsi, Y. (2008). Temperature dependence of silicon hardness: experimental evidence of phase transformations. Rev. Adv. Mater. Sci, 17(1-2), 3341.Google Scholar