The occurrence of artificial kalsilite and allied potassium aluminium silicates in blast-furnace linings

Published online by Cambridge University Press:  14 March 2018

G. R. Rigby
Affiliation:
British Refractories Research Association, Stoke-on-Trent
H. M. Richardson
Affiliation:
British Refractories Research Association, Stoke-on-Trent

Extract

The contour and dimensions of a typical blast furnace are shown in fig. 1. The shell of the furnace consists of riveted steel plates, inside which is a lining of firebricks varying in thickness about 2–3½ feet. Molten iron collects in the crucible or hearth at the bottom of the furnace and is periodically run off through a hole in the side of the furnace known as the tap-hole. The hearth is lined with firebrick both around the sides and along the floor, the total thickness of brickwork below the hearth in fig. 1 being 3 feet 9 inches.

Type
Research Article
Copyright
Copyright © The Mineralogical Society of Great Britain and Ireland 1947

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

page 76 note 1 Bannister, F. A. and Hey, M. H., Min. Mag., 1942, vol. 26, p. 218.CrossRefGoogle Scholar

page 80 note 1 Bowen, N. L., Amer. Journ. Sci., 1917, ser. 4, vol. 43, p. 115. [M.A. 1–167.]CrossRefGoogle Scholar

page 80 note 2 Thugutt, S. J., Arch. Min. Tow. Nauk. Warszaw., 1937, vol. 13, p. 112. [M.A. 7–146.]Google Scholar

page 88 note 1 Alfred Hartley Jay (1906–47) had been working on this same problem and this appendix contains his notes dated February 19, 1947. He died on February 26, 1947, after a motor-car accident on February 22. Two papers by him in this Magazine (1944, vol. 27, pp. 54 and 56) gave much promise of further useful work.