Hostname: page-component-76fb5796d-skm99 Total loading time: 0 Render date: 2024-04-28T22:23:53.506Z Has data issue: false hasContentIssue false

The Relationship of Porous Silicon Film Morphology to The Photoluminescence Spectra

Published online by Cambridge University Press:  25 February 2011

John Penczek
Affiliation:
Department of Electrical and Computer Engineering, University of California, Davis Davis, CA 95616
R. L. Smith
Affiliation:
Department of Electrical and Computer Engineering, University of California, Davis Davis, CA 95616
Get access

Abstract

Photoluminescence (PL) spectra are presented for porous silicon samples formed under various formation conditions in aqueous HF solutions. Formation conditions are chosen that effect maximal changes in morphology of resultant films and that correspond to varying formation electrochemistry. The trends in PL center wavelength and full width at half maximum (FWHM) with formation conditions are examined and compared to the resulting morphology. The PL spectra were observed to be most affected by changes in formation conditions when porous films are formed where the electrochemical process of silicon dissolution changes from a 2e- to 4e- (oxide production) reaction. Under these conditions, decreasing HF concentration and/or increasing current density produces a spectral blue-shift which is proportional to the narrowing of the FWHM. This behavior corresponds to morphology changes which are consistent with the quantum confinement model.

Type
Research Article
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

[1] Canham, L. T., Appl. Phys. Lett. 57, 1046 (1990)CrossRefGoogle Scholar
[2] Herino, R., Bomchil, G. et al. , J. Electrochem. Soc. 134, 1994 (1987)CrossRefGoogle Scholar
[3] Beale, M. I. J., Benjamin, J. D. et al. , J. Crystal Growth 73, 622 (1985)CrossRefGoogle Scholar
[4] Zhang, X. G., Collins, S. D., and Smith, R. L., J. Electrochem. Soc. 136, 1561 (1989)CrossRefGoogle Scholar
[5] Unno, H., Imai, K., and Muramoto, S., J. Electrochem. Soc. 134, 645 (1987)CrossRefGoogle Scholar
[6] Brumhead, D., Canham, L. T. et al. , Electrochimica Acta 38, 191 (1993)CrossRefGoogle Scholar
[7] Canham, L. T., Houlton, M. R. et al. , J. Appl. Phys. 70, 422 (1991)CrossRefGoogle Scholar
[8] Vial, J. C., Bsiesy, A. et al. , Phys. Rev. B 45, 14171 (1992)CrossRefGoogle Scholar
[9] Sanders, G.D. and Chang, Yia-Chung, Appl. Phys. Lett. 60, 2525 (1992)CrossRefGoogle Scholar
[10] Ohno, T., Shiraishi, K., and Ogawa, T., Phys. Rev. Lett. 69, 2400 (1992)CrossRefGoogle Scholar
[11] Smith, R. L., Chuang, S.-F., and Collins, S. D., J. Electron. Mat. 17, 533 (1988)CrossRefGoogle Scholar