Tribological Properties of Laser Deposited SiC Coatings

Published online by Cambridge University Press:  15 February 2011

T. Zehnder
Affiliation:
Institute of Applied Physics, University of Bern, Sidlerstr. 5, 3012 Bern, Switzerland
A. Blatter
Affiliation:
Institute of Applied Physics, University of Bern, Sidlerstr. 5, 3012 Bern, Switzerland
J. Burger
Affiliation:
Swiss Center for Electronics and Microtechnology, Inc., P.O. 41, CH-2007 Neuchâtel, Switzerland
C. Julia-Schmutz
Affiliation:
Swiss Center for Electronics and Microtechnology, Inc., P.O. 41, CH-2007 Neuchâtel, Switzerland
R. Christoph
Affiliation:
Swiss Center for Electronics and Microtechnology, Inc., P.O. 41, CH-2007 Neuchâtel, Switzerland
Get access

Abstract

We studied on a nanometer scale the tribological properties of thin silicon carbide films on Si(100) wafers and stainless steel. The coatings were fabricated from a sintered SiC target by pulsed ArF laser deposition at substrate temperatures between 20 °C and 1000 °C. Amorphous films resulted at low deposition temperatures while nanocrystalline structures developed at high deposition temperatures. An atomic force/lateral force microscope was employed to characterize the film topography and the friction behavior. The microhardness was determined from measurements utilizing a depth-sensing nanoindentation instrument. The SiC films on Si(100) exhibit a smooth surface with an average roughness Ra of a few nanometer, the amorphous films being even an order of magnitude smoother. No appreciable differences were found in microhardness and friction coefficient between amorphous and nanocrystalline films. On stainless steel, amorphous SiC coatings were obtained for deposition temperatures up to 500 °C. Their surface relief portrayed the grain boundaries of the underlying steel substrate, reflecting the ballistic nature of the deposition process. No stoichiometric films were obtained above 500 °C as the silicon from the growing film quickly dissolved in the steel substrate.

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Bhushan, Bharat and Gupta, B. K., Handbook of Tribology. 1st ed. (McGraw-Hill Inc., 1991), p. 14/73.Google Scholar
2. Ignat, M., Ducarroir, M., Lelogeais, M., Garden, J., Thin Solid Films 220, 271 (1992).CrossRefGoogle Scholar
3. Krishnaswamy, J., Rengan, A., Narayan, J., Vedam, K., McHargue, C. J., Appl. Phys. Lett. 54, 2455 (1989).Google Scholar
4. Zehnder, T., Blatter, A., Bächli, A., Thin Solid Films 241, 138 (1994).CrossRefGoogle Scholar
5. Notz Stahl AG, 2555 Brügg, Switzerland.Google Scholar
6. Marti, O., Physica Scripta T49, 599 (1993).CrossRefGoogle Scholar
7. Doener, M. F. and Nix, W. D., J. Mater. Res. 1 (4), 601 (1986).Google Scholar
8. Landolt Börnstein NS III/17a, (Springer-Verlag, Heidelberg, 1982), p. 77.Google Scholar
9. Jönsson, B. and Hogmark, S., Thin Solid Films 114, 257 (1984).CrossRefGoogle Scholar
10. Dupendant, H., Gavignan, J. P., Givord, D., Lienard, A., Rebouillat, J. P., Souche, Y., Appl. Surf. Sci. 43, 369 (1989).CrossRefGoogle Scholar