Hostname: page-component-76fb5796d-r6qrq Total loading time: 0 Render date: 2024-04-29T14:33:02.613Z Has data issue: false hasContentIssue false

Influence of Controlled Cooling Rates During Thermal Processing of Ti 6% Al 4% V Alloys Using In-Situ Scanning Electron Microscopy

Published online by Cambridge University Press:  13 April 2020

Genevieve A Kane*
Affiliation:
Department of Materials Science and Engineering Center for Materials, Devices and Integrated Systems, Rensselaer Polytechnic Institute, 110 8th Street Troy, NY, 12180
M. David Frey
Affiliation:
Center for Materials, Devices and Integrated Systems, Rensselaer Polytechnic Institute, 110 8th Street Troy, NY, 12180
Robert Hull
Affiliation:
Department of Materials Science and Engineering Center for Materials, Devices and Integrated Systems, Rensselaer Polytechnic Institute, 110 8th Street Troy, NY, 12180
Get access

Abstract

We describe experimental approaches to real time examination of the microstructural evolution of Ti 6%Al 4%V upon cooling from above the beta transus (~995 °C) while imaging in the scanning electron microscope. Ti 6%Al 4%V is a two phase, α+β titanium alloy with high strength and corrosion resistance. The β →α transformation on cooling can give rise to different microstructures and properties through various thermal treatments. Fully lamellar microstructures, bi-modal microstructures, and equiaxed microstructures can each be obtained by accessing different cooling rates upon the final treatment above the beta temperature, each resulting in uniquely enhanced material properties.

Utilizing the capabilities of a heating/ tensile stage developed by Kammrath & Weiss Inc., are able to apply real-time imaging techniques in the scanning electron microscope to monitor the development of the microstructure. Annealing temperatures up to 1100 °C are attainable, with cooling rates ranging from 0.1 ° C per second to 3.3 °C per second. This has allowed us to directly observe the formation of lamellae at different annealing temperature/ cooling rate combinations to determine the lamellar microstructure width, separation, and colony size.

Type
Articles
Copyright
Copyright © Materials Research Society 2020

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

References:

Gomez-Gallegos, A., Mandal, P., Gonzalez, D., Zuelli, N., and Blackwell, P., “Studies on Titanium Alloys for Aerospace Application,” Defect Diffus. Forum, vol. 385, pp. 419423, 2018.CrossRefGoogle Scholar
Banerjee, D. and Williams, J. C., “Perspectives on titanium science and technology,” Acta Mater., vol. 61, pp. 844879, 2013.CrossRefGoogle Scholar
Shi, X. H., Zeng, W. D., Shi, C. L., Wang, H. J., and Jia, Z. Q., “The effects of colony microstructure on the fatigue crack growth behavior for Ti-6A1-2Zr-2Sn-3Mo-1Cr-2Nb titanium alloy,” Mater. Sci. Eng. A, vol. 621, pp. 252258, 2015.CrossRefGoogle Scholar
Porter, D. A., Easterling, K. E., and Sherif, M. Y., Phase Transformations in Metals and Alloys, Third Edition. 2009.Google Scholar
Semiatin, S. L., Seetharaman, V., and Weiss, I., “Hot workability of titanium and titanium aluminide alloys—an overview,” Mater. Sci. Eng. A, vol. 243, no. 1–2, pp. 124, 2002.10.1016/S0921-5093(97)00776-4CrossRefGoogle Scholar
Lütjering, G., “Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys,” Mater. Sci. Eng. A, vol. 243, no. 1–2, pp. 3245, 1998.CrossRefGoogle Scholar
Poondla, N., Srivatsan, T. S., Patnaik, A., and Petraroli, M., “A study of the microstructure and hardness of two titanium alloys: Commercially pure and Ti-6Al-4V,” J. Alloys Compd., vol. 486, no. 1–2, pp. 162167, 2009.CrossRefGoogle Scholar
Semiatin, S. L., Knisley, S. L., Fagin, P. N., Zhang, F., and Barker, D. R., “Microstructure evolution during alpha-beta heat treatment of Ti-6Al-4V,” Metall. Mater. Trans. A Phys. Metall. Mater. Sci., vol. 34, no. 10, pp. 23772386, 2003.CrossRefGoogle Scholar
Patil, S.et al., “Effect of α and β Phase Volume Fraction on Machining Characteristics of Titanium Alloy Ti6Al4V,” Procedia Manuf., vol. 6, pp. 6370, 2016.CrossRefGoogle Scholar
Hayes, B. J.et al., “Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition,” Acta Mater., vol. 130, no. July, pp. 120133, 2017.Google Scholar
Shademan, S., Sinha, V., Soboyejo, A. B. O., and Soboyejo, W. O., “An investigation of the effects of microstructure and stress ratio on fatigue crack growth in Ti-6Al-4V with colony α/β microstructures,” Mech. Mater., vol. 36, pp. 161175, 2004.CrossRefGoogle Scholar
Ma, Y.et al., “Fatigue crack tip plastic zone of α + β titanium alloy with Widmanstatten microstructure,” J. Mater. Sci. Technol., vol. 34, no. 11, pp. 21072115, 2018.CrossRefGoogle Scholar
Zhang, X., Martina, F., Ding, J., Wang, X., and Williams, S. W., “Fracture toughness and fatigue crack growth rate properties in wire + arc additive manufactured Ti-6Al-4V,” Fatigue Fract. Eng. Mater. Struct., vol. 40, no. 5, pp. 790803, 2017.CrossRefGoogle Scholar
Chan, K. S. and Koss, D. A., “Fracture toughness of Widmanstatten colonies of an α-β titanium alloy,” Mater. Sci. Eng., vol. 43, no. 2, pp. 177186, 1980.CrossRefGoogle Scholar
Boehlert, C. J., Cowen, C. J., Tamirisakandala, S., McEldowney, D. J., and Miracle, D. B., “In situ scanning electron microscopy observations of tensile deformation in a boron-modified Ti–6Al–4V alloy,” Scr. Mater., vol. 55, no. 5, pp. 465468, 2006.CrossRefGoogle Scholar
Alabort, E., Putman, D., and Reed, R. C., “Superplasticity in Ti-6Al-4V: Characterisation, modelling and applications,” Acta Mater., vol. 95, pp. 428442, 2015.CrossRefGoogle Scholar
Brice, D. A.et al., “Oxidation behavior and microstructural decomposition of Ti-6Al-4V and Ti-6Al-4V-1B sheet,” Corros. Sci., vol. 112, pp. 338346, 2016.CrossRefGoogle Scholar