Synthesis and characterization of ceramic (Sr1−xCax)2 CuO3

Published online by Cambridge University Press:  31 January 2011

Ming Xu
Affiliation:
Ames Laboratory, United States Department of Energy, Department of Physics, and Department of Materials Science and Engineering, Iowa State University, Ames, Iowa 50011
E.T. Voiles
Affiliation:
Ames Laboratory, United States Department of Energy, Department of Physics, and Department of Materials Science and Engineering, Iowa State University, Ames, Iowa 50011
L.S. Chumbley
Affiliation:
Ames Laboratory, United States Department of Energy, Department of Physics, and Department of Materials Science and Engineering, Iowa State University, Ames, Iowa 50011
A.I. Goldman
Affiliation:
Ames Laboratory, United States Department of Energy, Department of Physics, and Department of Materials Science and Engineering, Iowa State University, Ames, Iowa 50011
D.K. Finnemore
Affiliation:
Ames Laboratory, United States Department of Energy, Department of Physics, and Department of Materials Science and Engineering, Iowa State University, Ames, Iowa 50011
Get access

Abstract

Ceramic (Sr1−xCax)2CuO3 samples have been prepared with x = 0.00, 0.25, 0.50, 0.55, 0.75, and 1.00 in order to study the change in lattice constants with the ratio of Sr/Ca. This phase is frequently an impurity phase in the fabrication of Bi–Sr–Ca–Cu–O superconductors, and it is important to be able to connect the lattice constants with stoichiometry. The behavior of the lattice constants closely follows Vegard's law.

Type
Articles
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Polonka, J., Xu, M., Goldman, A. I., Finnemore, D. K., and Li, Q., Supercond. Sci. Technol. (1991, in press).Google Scholar
2.Roth, R. S., Rawn, C. J., Whitler, J. D., Chiang, C. K., and Wong-Ng, W. K., J. Am. Ceram. Soc. 72 (3), 395399 (1989).CrossRefGoogle Scholar
3.Roth, R. S., Rawn, C. J., Ritter, J. J., and Burton, B. P., J. Am. Ceram. Soc. 72 (8), 15451549 (1989).CrossRefGoogle Scholar
4.Schulze, K., Majewaki, P., Hettich, B., and Petzow, G., Metallk, Z.. (in press).Google Scholar
5.Majewaki, P., Hettich, B., Kaeger, H., and Schulze, K., Adv. Mater, (in press).Google Scholar
6.Shi, D., Boley, M. S., Welp, U., Chen, J., and Laio, Y., Phys. Rev. B 40 (7), 52555258 (1989).CrossRefGoogle Scholar
7.Polonka, J., Xu, M., Li, Q., Finnemore, D. K., and Goldman, A. I., Appl. Phys. Lett. 59, 3640 (1991).CrossRefGoogle Scholar
8.Gadalla, A. M. M. and White, J., Trans. Br. Ceram. Soc. 65 (4), 181190 (1966).Google Scholar
9.Teske, G. L. and Müller-Buschbaum, H. H., Z. Anorg. Allg. Chem. 371, 325 (1969); 379, 234 (1970).CrossRefGoogle Scholar
10.Breuer, K-H., Eysel, W., and Behruzi, M., Z. Kristallogr. 176, 216 (1986).Google Scholar