Direct Observation of Single Atoms in Sinter-Resistant and Bimetallic Catalyst Systems Synthesized by Atomic Layer Deposition

Published online by Cambridge University Press:  09 October 2013

K.-B. Low
Affiliation:
Y. Lei
Affiliation:
J. Lu
Affiliation:
J.W. Elam
Affiliation:

Abstract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2013 in Indianapolis, Indiana, USA, August 4 – August 8, 2013.