Abstract
ABSTRACT

Neutron scattering experiments have been carried out with undeformed and creep deformed samples of the superalloy CMSX-4. From the measured constrained misfit data, obtained from different reflecting planes with respect to the external load axis, two strain tensors for horizontal and vertical matrix plates can be extracted.

A careful data analysis is necessary since the technical manufactured single crystals show a mosaic spreading of 0.5° and the wavelength spreading of the incident neutron beam, Δλ/λ is about 410-3 This is in the same range as the unknown constrained misfit quantities δc. A method has been developed which allows a calculated intensity distribution to be fitted to the measured one.

Copyright
References
Hide All
1 Frazier D.J., Whetstone J.R., Harris K., Erickson G.L. and R.E Schwer, High Temperature Materials for Power Engineering, Cost 501/505 Conf., Liège (1990)
2 Glatzel U., Microstructure and Internal Strains of Undeformed and Creep Deformed Samples of a Nickel-Base Superalloy (Verlag Köster, Berlin, 1994), ISBN 3-929937-91-3
3 Glatzel U. and Müller A., Scripta Met. Mat. 31, 285 (1994)
4. Glatzel U., Scripta Met. Mat. 31, 291 (1994)
5 Glatzel U. and Müller A., Numerical Predictions of Deformation Processes and the Behaviour of Real Materials, edited by Andersen S.I. et al. , (Riso National Laboratory, Roskilde, Denmark, 1994), 319
6 Müller L., Glatzel U. and Feller-Kniepmeier M., Acta Met. Mat. 41, 3401 (1993)
7 Schmidt R. and Feller-Kniepmeier M., Scripta Met. Mat. 29, 1079 (1993)
Recommend this journal

Email your librarian or administrator to recommend adding this journal to your organisation's collection.

MRS Online Proceedings Library (OPL)
  • ISSN: -
  • EISSN: 1946-4274
  • URL: /core/journals/mrs-online-proceedings-library-archive
Please enter your name
Please enter a valid email address
Who would you like to send this to? *
×

Metrics

Full text views

Total number of HTML views: 0
Total number of PDF views: 1 *
Loading metrics...

Abstract views

Total abstract views: 44 *
Loading metrics...

* Views captured on Cambridge Core between September 2016 - 23rd January 2018. This data will be updated every 24 hours.