Hostname: page-component-68c7f8b79f-rgmxm Total loading time: 0 Render date: 2025-12-24T01:23:59.187Z Has data issue: false hasContentIssue false

Fracture Analysis of Nodular Cast Iron By X-ray Fractography

Published online by Cambridge University Press:  06 March 2019

Kazuyuki Matsui
Affiliation:
Ishikawa Seisakusyo, LTD. Minamimorimoto Kanazawa, 92U-UI, Japan
Yukio Hirose
Affiliation:
Faculty of Material Science, Kanazawa University 1-1, Marunouchi, Kanazawa 920, Japan
Akiyoshi Chadani
Affiliation:
Faculty of Material Science, Kanazawa University 1-1, Marunouchi, Kanazawa 920, Japan
Keisuke Tanaka
Affiliation:
Faculty of Engineering Science, Kyoto University Yoshida Honmachi, Sakyo-ku, Kyoto, Japan
Get access

Extract

Fracture accidents of engineering structures and machines in operation sometimes result from defects. One of the purposes of fracture analysis are to determine the causes of failure, and to use the information to prevent similar failure accidents. It is important to obtain quantitative analysis from the fracture surface. X-ray diffraction technique as well as Electron Fraotography has been widely used for fracture analysis of engineering structures and machines.

Information

Type
XII. Analysis of Stress and Fracture by Diffraction Methods
Copyright
Copyright © International Centre for Diffraction Data 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Matsui, K., Hirose, Y., Chadani, A., Tanaka, K., “X-Ray Fractographic Study on Fracture of a Machine Part”, 2nd International Conference on Residual Stress. 833 (1989)Google Scholar
2. Matsui, K., Hirose, Y., Chadani, A., Tanaka, K., “X-Ray Fractography and Its Application to Failure Analysis”, J. Soci. Mat. Sci. Jap., 39:614(1990)Google Scholar
3. Hirose, Y., Tanaka, K., “X-Ray Measurement of Residual Stress near Fatigue Fracture Surfaces of High Strength Steel”, Advances in X-Ray Analysis. 29:265(1986)10.1154/S0376030800010351Google Scholar
4. Matsui, K., Hirose, Y., Yajima, Z., Tanaka, K., “X-Ray Fractography on Fracture Surface by Failure of Ductile Cast Iron” X-ray Studies on Mechanical Behavior of Materials. 101(1988)Google Scholar
5. Lian, P. K., Landes, J. D., “Influence of Prestrain History on Fracture Toughness Properties of Steels” Metallurgical Trans., 17A:473(1986)Google Scholar
6. Levy, N., Marcal, P. V., Ostengren, W. J., Rice, J. R., “Small Scale Yielding near a Crack in Plane Strain: A Finite Analysis”, Int. J. Frac., 7:143(1971)Google Scholar