Hostname: page-component-68c7f8b79f-m4fzj Total loading time: 0 Render date: 2025-12-20T05:36:21.842Z Has data issue: false hasContentIssue false

The Study of Fatigue Behavior of Ductile Cast Iron by Means of X-Ray Fractographic Technique

Published online by Cambridge University Press:  06 March 2019

Zenjiro Yajima
Affiliation:
Department of Mechanical Engineering, Kanazawa Institute of Technology, 7-1 Oogigaoka, Nonoiehi, Kanazawa 921, Japan
Masaki Shinohara
Affiliation:
NEC Corporation, Tamagawa Plant, 1753, Shimonumabe Nakahara-ku, Kawasaki, Kanagawa 211, Japan
Ken-ichi Ishikawa
Affiliation:
Department of Mechanical Engineering, Kanazawa Institute of Technology, 7-1 Oogigaoka, Nonoichi, Kanazawa 921, Japan
Yukio Hirose
Affiliation:
Department of Materials Science, Kanazawa University 1-1 Marunouchi, Kanazawa 920, Japan
Keisuke Tanaka
Affiliation:
Department of Mechanical Engineering, Nagoya University Furoh-cho, Chigusa-ku, Nagoya 464-01, Japan
Get access

Extract

X-ray diffraction observation of metal fractures provides fracture analysis with useful information on the mechanisms and mechanical conditions of fracturing. This method is called “X-ray fractography” and has been developed especially in Japan as a new engineering tool for fracture analysis.

Information

Type
VII. Stress Determination by Diffraction Methods
Copyright
Copyright © International Centre for Diffraction Data 1991

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Yajima, Z., Hirose, Y., and Tanaka, K., “X-Ray Examination of Fracture Surfaces of Silicon Nitride Ceramics,” Advances in X-Ray Analysis, 33:319 (1990).Google Scholar
2. Yajima, Z., Shimazu, Y., Ishikawa, K., Hirose, Y., and Tanaka, K., “X-Ray Fractographic Study on Fracture Surface Made by Fatigue Crack Propagation Tests of Ductile Cast Iron,” Journal of The Japanese Society for Strength and Fracture of Materials, 22:121 (1988).Google Scholar
3. Yajima, Z., Hirose, Y., and Tanaka, K., X-Ray Fractography of Fatigue Fracture of Low-Alloy Steel in Air and in 3.5% NaCl Solution,” Journal of The Society of Materials Science Japan, 35:725 (1986).Google Scholar
4. Hirose, Y., Yajima, Z., and Tanaka, K.,“X-Ray Fractographic Approach to Fracture Toughness of AISI 4340 Steel,” Advances in X-Ray Analysis, 28:289 (1985).Google Scholar
5. Levy, N., Marcal, P.V., Ostengren, W.J., and Rice, J.R., “Small Scale Yielding Near A Crack in Plane Strain: A Finite Element Analysis,” International Journal of Fracture, 7:143 (1971).Google Scholar