Hostname: page-component-857557d7f7-nbs69 Total loading time: 0 Render date: 2025-12-08T02:17:19.411Z Has data issue: false hasContentIssue false

Development of mechanical tests for stress corrosion and fatigue corrosion studies

Published online by Cambridge University Press:  25 October 2002

Get access

Abstract

Two specific examples are presented to describe the experience gained in the use of mechanical tests for the study of stress corrosion cracking and corrosion-fatigue: 1) the design of tension test platforms and low-frequency fatigue machines, having cross-head displacement rates of the order of 1 μm/h; 2) the use of curved tension test pieces to take into account heterogeneities of the material microstructure, in the case of cracking phenomena in burried pipelines.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2002

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable