High temperature evolution of the microstructure of a cast cobalt base superalloy - Consequences on its thermomechanical properties

Published online by Cambridge University Press:  06 October 2004

Get access

Abstract

The prolonged holding at high temperature of certain cast cobalt base superalloys may lead to rarefaction and fragmentation of the tantalum carbides which harden these alloys. Room temperature hardness, thermal dilatation and high temperature tensile strength have been studied in relation with these processes. Only the thermal dilatation coefficient and the modulus of elasticity are really affected by the evolution of the tantalum carbides.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable