Hostname: page-component-7dd5485656-c8zdz Total loading time: 0 Render date: 2025-10-31T09:17:15.365Z Has data issue: false hasContentIssue false

C, Si and Sn Implantation of CVD Diamond as a means of Enhancing Subsequent Etch Rate

Published online by Cambridge University Press:  01 February 2011

P. W. Leech
Affiliation:
CSIRO Manufacturing and Infrastructure Technology, Clayton, Victoria, Australia.
T. Perova
Affiliation:
Dept. of Electronic and Electrical Engineering, University of Dublin, Trinity College, Ireland.
R. A. Moore
Affiliation:
Dept. of Electronic and Electrical Engineering, University of Dublin, Trinity College, Ireland.
G. K. Reeves
Affiliation:
RMIT University, School of Computer Systems and Elect. Eng., Melbourne, Australia.
A. S. Holland
Affiliation:
RMIT University, School of Computer Systems and Elect. Eng., Melbourne, Australia.
M. Ridgway
Affiliation:
Dept. of Electronic Materials Engineering, ANU, Canberra, Australia.
Get access

Abstract

Diamond films were implanted with C+, Si+ or Sn+ ions at multiple energies in order to generate a uniform region of implantation-induced disorder. Analysis of the C+ implanted surfaces by micro-Raman spectroscopy has shown only minor increase in the proportion of nondiamond or sp2-bonded carbon at doses of 5 × 1013 - 5 × 1015 ions/cm2. In comparison, an amorphization of the structure was evident after implantation with either Si+ ions at a dose of 5 × 1015 ions/cm2 or with Sn+ ions at >5 × 1014 ions/cm2. At a given implantation dose, the etch rate of the diamond film in a CF4/O2 plasma increased with the mass of the implanted species in the order of C+, Si+ and Sn+. For a given implant species, the etch rate was directly proportional to vacancy concentration as controlled by the dose or the implantation-induced disorder.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Malshe, A.P., Park, B.S., Brown, W.D. and Naseem, H.A., Diamond Rel. Mater. 8, 1198 (1999).Google Scholar
2. Vivensang, C., Ferlazzo-Manin, L., Ravet, M.V., Turban, G., Rosseaux, F. and Gicquel, A., Diamond Rel. Mater., 5, 840 (1996).Google Scholar
3. Leech, P.W., Reeves, G.K. and Holland, A.S., Journal Materials Science, 36, 3453 (2001).Google Scholar
4. Prawer, S., Hoffman, A and Kalish, R., Appl. Phys. Lett. 57 (21) (1990) 2187.Google Scholar
5. Prawer, S., Kalish, R., Phys. Rev., B51, (1995), 15711.Google Scholar
6. Jiang, N., Deguchi, M., Wang, C.L., Won, J.H., Jeon, H.M., Mori, Y., Hatta, A., Kitabatake, M., Ito, T., Hirao, T., Sasaki, T. and Hiraki, A., Appl. Surf. Sci. 113/114 (1997) 254.Google Scholar
7. Sun, Z., Shi, J.R., Tay, B.K. and Lau, S.P., Diamond Rel. Mater. 9 (2000) 1979.Google Scholar
8. Sato, S. and Iwaki, M., Nuclear Instruments Methods in Physics Res., B32, 145 (1988).Google Scholar
9. Avigal, Y., Richter, V., Fizgeer, B., Saguy, C. and Kalish, R., Diamond Rel. Mater. 13 (2004) 1674.Google Scholar
10. Steinbruchel, C., Appl. Phys. Lett. 55(19) (1989) 1960.Google Scholar
11. Steinbruchel, C., MRS Symp. Proc. Laser and particle beam chemical processes on surfaces, Pittsburgh PA, 129, 477 (1989).Google Scholar
12. Kobayashi, K., Mutsukura, N. and Machi, Y., Thin Solid Films, 200, 139 (1991).Google Scholar
13. Prins, J.F., Mater. Sci.Eng., B11, 219 (1992).Google Scholar