Hostname: page-component-7857688df4-4hfp6 Total loading time: 0 Render date: 2025-11-13T04:03:50.119Z Has data issue: false hasContentIssue false

Determination Of Intermetallic Formation Mechanism Using Differential Scanning Calorimetry Of Multilayered Thin Films

Published online by Cambridge University Press:  25 February 2011

T. E. Schlesinger
Affiliation:
Department of Materials Science and Engineering, The Johns Hopkins University, Baltimore, MD 21218
S. M. Prokes
Affiliation:
Naval Research Laboratory, Washington, D.C. 20375
R. C. Cammarata
Affiliation:
Department of Materials Science and Engineering, The Johns Hopkins University, Baltimore, MD 21218
Get access

Abstract

The ability to determine which growth mechanism (interface-reaction-rate-limited vs. diffusion-limited) of intermetallic formation by interfacial reactions using differential scanning calorimetry (DSC) is demonstrated. Suicide formation in multilayered thin films of chromium and amorphous silicon was chosen as a model system. It is shown that suicide formation in this system followed a linear rate law corresponding to an interface-reaction-rate-limited growth mechanism. An activation energy and pre-exponential for the rate constant were determined.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Highmore, R.J., Evetts, J.E., Somekh, R.E., and Greer, A.L., Appl. Phys. Lett. j 50, 566 (1987).Google Scholar
2. Clevenger, L.A., Thompson, C.V., Cammarata, R.C., and Tu, K.N., Appl. Phys. Lett. 52, 795 (1988).Google Scholar
3. Clevenger, L.A., Thompson, C.V., Cammarata, R.C., and Tu, K.N., Mater. Res. Soc. Symp. Proc. Vol. 103. 191 (1988).Google Scholar
4. Clevenger, L.A., Thompson, C.V., Judas, A.D., and Tu, K.N., Mater. Res. Soc. Internat. Meeting Adv. Mater. 10, 431 (1989).Google Scholar
5. Clevenger, L.A., Ph.D. Thesis, Massachusetts Institute of Technology, 1989.Google Scholar
6. Schlesinger, T.E., Cammarata, R.C., and Prokes, S.M., Appl. Phys. Lett. 59, 449 (1991).Google Scholar
7. Kissinger, H.E., Anal. Chem. 29., 1702 (1957).Google Scholar