Determining the Area Function of Spherical Indenters for Nanoindentation.

Published online by Cambridge University Press:  17 March 2011

Andrew J. Bushby
Affiliation:
Department of Materials, Queen Mary, University of London, UNITED KINGDOM
Nigel M. Jennett
Affiliation:
NPL Materials Centre, National Physical Laboratory, Teddington, UNITED KINGDOM
Get access

Abstract

Nanoindentation with spherical tipped indenters provides a powerful technique for exploring surface mechanical properties through the application of Hertzian mechanics. The full range of mechanical response can be obtained from elastic, through the yield point to a range of permanent deformation. However, the successful application of the technique requires accurate calibration of the indenter tip geometry. In this paper methods based on indentation into a number of reference materials are used to characterise a range of spherical tipped indenters with nominal radii from 5 to 50 microns. A traceably calibrated metrological AFM is also used to determine the actual shape of one of the indenters. The sensitivity of each method to test parameters is discussed. Coincidence of the data from both methods validates the determined shape of the indenter and offers the opportunity to cross-correlate the calibration of both instruments with high sensitivity.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Lawn, B.R., J. Am. Ceram. Soc., 81, 19771994, (1998)Google Scholar
2. Bushby, A.J., “Nano-Indentation Using Spherical Indenters”, accepted for publication in Nondest. Test. and Eval., 2000.Google Scholar
3. Bushby, A.J., “Physical Origin of a Size Effect in Nanoindentation” this volume.Google Scholar
4. Field, J.S. and Swain, M.V., J. Mater. Res., 8, 297306. (1993)Google Scholar
5. Oliver, W.C. and Pharr, G.M., J. Mater. Res., 7, 15641583, (1992)Google Scholar
6. Herrmann, K. and Jennett, N.M.Progress in determination of area function of indenters used for nanoindentation” Proc ICMCTF2000, San Diego (to be published in Thin Solid Films)Google Scholar
7. Johnson, K.L., “Contact Mechanics”, Cambridge University Press, (1985)Google Scholar
8. Jennett, N M; Shafirstein, G; Saunders, S R J. in Hardness Testing in Theory and Practice Proc. 9th Int. Symp. Hardness Testing in Theory and Practice, Düsseldorf, Nov 1995 VDI Berichte, 1194 pp201-210 Publ. VDI-Verlag GmbH, Dusseldorf, (1995)Google Scholar
9. Jennett, Nigel M and Meneve, Jan; Mat Res Soc. Symp Proc. 522, 239244, (1998)Google Scholar