Hostname: page-component-68c7f8b79f-qcl88 Total loading time: 0 Render date: 2025-12-20T00:08:13.239Z Has data issue: false hasContentIssue false

Finite Element Modeling of Nanoindentation Measurements of Crystalline and Amorphous Si

Published online by Cambridge University Press:  17 March 2011

J. A. Knapp
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185-1056
D. M. Follstaedt
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185-1056
S. M. Myers
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185-1056
G. A. Petersen
Affiliation:
Sandia National Laboratories, Albuquerque, NM 87185-1056
Get access

Abstract

Nanoindentation testing of amorphous Si layers, formed by self-ion implantation, has been performed, and their mechanical properties compared to crystalline Si. The data was analyzed using finite element modeling of the indentation measurement, allowing the properties of the thin amorphous layers to be separated from those of the underlying material. By modeling the materials as isotropic, elastic-plastic solids with the Mises yield criterion, the amorphous Si is shown to have a hardness about 15% lower than crystalline Si and an elastic modulus about 10% lower. Electron and atomic force microscopies of the indents indicate that the amorphous Si does not undergo phase changes during indentation, and that it may be somewhat more ductile than crystalline Si.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Clarke, D.R., Kroll, M.C., Kirchner, P.D., Cook, R.F. and Hockey, B.J., Phys. Rev. Lett. 60, 2156 (1988).Google Scholar
2. Pharr, G.M., Mat. Res. Soc. Symp. Proc. 239, 301 (1992).Google Scholar
3. Mann, A.B., Heerden, D. van, Pethica, J.B., and Weihs, T.P., J. Mater. Res. 15, 1754 (2000).Google Scholar
4. Knapp, J.A., Follstaedt, D.M., Myers, S.M., Barbour, J.C. and Friedmann, T.A., J. Appl. Phys. 85, 1460 (1999).Google Scholar
5. Szabadi, M., Hess, P., Kellock, A.J., Coufal, H., and Baglin, J.E.E., Phys. Rev. B58, 8941 (1998).Google Scholar
6. Custer, J.S., Thompson, Michael O., Jacobson, D.C., Poate, J.M., Roorda, S., Sinke, W.C. and Spaepen, F., Appl. Phys. Lett. 64, 437 (1994).Google Scholar
7. Follstaedt, D.M., Knapp, J.A., Myers, S.M. and Petersen, G.A., Mat. Res. Soc. Symp. Proc. 557, to be published.Google Scholar
8. Oliver, W. C. and Pharr, G. M., J. Mater. Res. 7, 1564 (1992).Google Scholar
9. All of the indentation tests were performed at the MTS Systems Corp., Knoxville, TN.Google Scholar
10. ABAQUS version 5.8, Hibbitt, Karlsson & Sorensen, Inc., Pawtucket, RI.Google Scholar
11. Hirth, J.P. and Lothe, J., Theory of Dislocations (Krieger, Malabar, FL, 1992), pp. 426-428, 836.Google Scholar