Finite Element Studies of the Influence of Pile-up on the Analysis of Nanoindentation Data

Published online by Cambridge University Press:  15 February 2011

A. Bolshakov
Affiliation:
Department of Materials Science, Rice University, 6100 Main St., Houston, TX 77005
W. C. Oliver
Affiliation:
Nano Instruments, Inc., 1001 Larson Drive, Oak Ridge, TN 37830
G. M. Pharr
Affiliation:
Department of Materials Science, Rice University, 6100 Main St., Houston, TX 77005
Get access

Abstract

Methods currently used for analyzing nanoindentation load-displacement data give good predictions of the contact area in the case of hard materials, but can underestimate the contact area by as much as 40% for soft materials which do not work harden. This underestimation results from the pile-up which forms around the hardness impression and leads to potentially significant errors in the measurement of hardness and elastic modulus. Finite element simulations of conical indentation for a wide range of elastic-plastic materials are presented which define the conditions under which pile-up is significant and determine the magnitude of the errors in hardness and modulus which may occur if pile-up is ignored. It is shown that the materials in which pile-up is not an important factor can be experimentally identified from the ratio of the final depth after unloading to the depth of the indentation at peak load, a parameter which also correlates with the hardness-to-modulus ratio.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, p. 1564 (1992).Google Scholar
2. Sneddon, I.N., Int. J. Engng. Sci. 3, p. 47 (1965).Google Scholar
3. Bolshakov, A., Oliver, W.C. and Pharr, G.M., J. Mater. Res. 11, p. 760 (1996).Google Scholar
4. Tabor, D., in Microindentation Techniques in Materials Science and Engineering, ASTM STP 889, Blau, P.J. and Lawn, B.R., Eds., American Society for Testing and Materials, Philadelphia, 1986, pp. 129159.Google Scholar
5. Bolshakov, A. and Pharr, G.M., submitted to this conference proceedings.Google Scholar
6. Bolshakov, A., Oliver, W.C. and Pharr, G.M., to be published.Google Scholar