Multiscale Characterization of Deformation Mechanisms in the Weld Joint of a Nickel-based Superalloy

Published online by Cambridge University Press:  01 February 2011

O.M. Barabash
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
J.A. Horton
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
S.S. Babu
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
J.M. Vitek
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
S.A. David
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
G.E. Ice
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
R.I. Barabash
Affiliation:
Metals and Ceramics Div., Oak Ridge National Laboratory, Oak Ridge, TN
Get access

Abstract

Multiscale plastic deformation in the heat affected zone (HAZ) of a Ni-based single crystal superalloy has been characterized using white microbeam synchrotron diffraction measurements together with OIM imaging, electron and optical microscopy. Characteristic length scales on the macro, meso and nano scale are determined. Dissolution of the γ' – phase particles during heating and secondary precipitation of γ' – phase during cooling is found, as well as formation and multiplication of dislocations. This process is more intense as one approaches the fusion line (FL). In the regions immediately neighboring the FL, γ' - phase particles dissolve completely and reprecipitate from the solid solution in the form of very small (50-70nm) particles. In the immediate vicinity of the FL, the temperature gradient and the rate of it's change reaches maximal values and causes the formation of large amounts of dislocations. Dislocations are concentrated in the ã matrix of the single crystal superalloy. X-ray Laue diffraction (both conventional and microbeam) and electron microscopy show that alternating dislocations slip systems dominate in the HAZ with typical Burgers vector b=[110]. Local lattice rotations in different zones of the weld joint are linking with the microslip events in different zones of the weld.

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Dye, D., Hunziker, O., Roberts, S.M., and Reed, R.C., Metallurgical and Mater. Trans. A, 32, (2001) 17131725 Google Scholar
2 Barabash, O., Babu, S., David, S., Vitek, J., Barabash, R., J. Appl. Physics, 93, 13, (2003).Google Scholar
3 Park, J.-W., Vitek, J.M., Babu, S.S., David, S.A.. Submitted to Science and Technology of Welding and JoiningGoogle Scholar
4 Larson, B.C., Yang, Wenge, Ice, G.E., Budai, J.D., Tischler, J.Z., Nature, 415, 887, (2002).Google Scholar
5 Barabash, R., Ice, G.E., Walker, F., J. Appl. Physics, 93, 3, 14571464 (2003)Google Scholar
6ABAQUS, ver.6.3-1, HKS. 2003Google Scholar
7 Dye, D., Hunziker, O., Reed, R.C., Metallurgical and Materials Transaction A, 2001, 32A, p17131725 Google Scholar
8 Sundman, B., Jansson, B. and Andersson, J-O., “The ThermoCalc Database System”, Calphad, 9, 1985, 153190 Google Scholar
9 , Ni-DATA, v.5, Saunders, N., ThermoTech Ltd., Surrey Technology Centre, 40 Occam Road, GuildfordGU2 5YH, United Kingdom, (2001)Google Scholar