Nanoindentation Hardness of Soft Films on Hard Substrates: Effects of the Substrate

Published online by Cambridge University Press:  10 February 2011

T. Y. Tsui
Affiliation:
Advanced Micro Devices, One AMD Place, MS 32, P.O. Box 3453, Sunnyvale, CA 94088
C. A. Ross
Affiliation:
Department of Materials Science and Engineering, Massachusetts Institute of Technology, 13–4005, 77 Mass Ave., Cambridge, MA 02139
G. M. Pharr
Affiliation:
Department of Materials Science, Rice University, 6100 Main St., MS 321, Houston, TX 77005–1892
Get access

Abstract

The ability to accurately measure the mechanical properties of thin metallic films is important in the semiconductor industry as it relates to device reliability issues. One popular technique for measuring thin film mechanical properties is nanoindentation. This technique has the advantage of being able to measure properties such as hardness and elastic modulus without removing a film from its substrate. However, according to a widely-held rule of thumb, intrinsic film properties can be measured in a manner which is not influenced by the substrate only if the indentation depth is kept to less than 10% of the film thickness, which is often not practical. In this work, a method for making substrate independent hardness measurements of soft metallic films on hard substrates is proposed. The primary issue to be addressed is the substrate-induced enhancement of indentation pile-up and the ways in which this pile-up influences the contact area determined from analyses of nanoindentation load-displacement data. Based on experimental observations of soft aluminum films on silicon, glass, and sapphire substrates, a simple empirical relationship is derived which relates the amount of pile-up to the contact depth. From this relationship, a simple method is developed which allows the intrinsic hardness of the film to be measured by nanoindentation methods even when the indenter penetrates through the film into the substrate.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1997

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Tsui, T.Y., Oliver, W.C., and Pharr, G.M., J. Mater. Res. 11, 752 (1996).Google Scholar
2. Tsui, T.Y., Oliver, W.C., and Pharr, G.M., Mater. Res. Soc. Symp. Proc. 436, 207 (1996).Google Scholar
3. Laursen, T.A. and Simo, J.C., J. Mater. Res. 7, 618 (1992).Google Scholar
4. Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, 1564 (1992).Google Scholar
5. Tsui, T.Y., Bolshakov, A., and Pharr, G.M., in preparation.Google Scholar
6. Stone, D., LaFontaine, W.R., Alexopoulos, P., Wu, T.W., and Li, C.-Y., J. Mater. Res 3, 141 (1988).Google Scholar
7. LaFontaine, W.R., Yost, B., and Li, C.-Y., J. Mater. Res. 5, 776 (1990).Google Scholar
8. Bhattacharya, A.K. and Nix, W.D., Int. J. Solid Structure 24, 1287 (1988).Google Scholar
9. Burnett, P.J. and Rickerby, D.S., Thin Solid Film 148, 41 (1987).Google Scholar
10. Burnett, P.J. and Rickerby, D.S., Thin Solid Films 148, 51 (1987).Google Scholar
11. Jonsson, B. and Hogmark, S., Thin Solid Films 114, 257 (1984).Google Scholar