A scanning tunneling microscopy (STM) study of low load indentations into Si, GaAs and Au is presented. Compared with standard micrographs obtained through optical microscopy and scanning electron microscopy, the STM images show greatly improved resolution in and around the indentation. The effects of relaxation and pile-up may be observed through contour plots which show inward bowing of the indentation faces in Si.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Castell, M.R., Walls, M.G. and Howie, A., presented at the STM '91 conference in Interlaken, to be published in Ultramicroscopy, May '92.Google Scholar
2. Takahagi, T., Nagai, I., Ishitani, A., Kuroda, H. and Nagasawa, Y., J. Appl. Phys. 64. 3516(1988).Google Scholar
3. Hu, J.Z., Merkle, L.D., Menoni, C.S. and Spain, I.L., Phys. Rev. B, 24. 4679 (1986).CrossRefGoogle Scholar
4. Ericson, F., Johansson, S. and Schweitz, J-A, Mat. Sci. and Eng. A, 105/106. 131 (1988).Google Scholar
5. Clarke, D.R., Kroll, M.C., Kirchner, P.D. and Cook, R.F., Phys. Rev. Lett. 60, 2156 (1988).Google Scholar
6. Hirsch, P.B., Pirouz, P., Roberts, S.G. and Warren, P.G., Phil. Mag. B, 52 (3), 759 (1985).Google Scholar