Hostname: page-component-68c7f8b79f-tw422 Total loading time: 0 Render date: 2025-12-24T05:11:28.067Z Has data issue: false hasContentIssue false

Size Effect Characterization for Nanostructured Material in Nanoindentation Test

Published online by Cambridge University Press:  01 February 2011

Yueguang Wei
Affiliation:
LNM, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, P.R. China
Ying Du
Affiliation:
LNM, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, P.R. China
Siqi Shu
Affiliation:
LNM, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, P.R. China
Chen Zhu
Affiliation:
LNM, Institute of Mechanics, Chinese Academy of Sciences, Beijing 100080, P.R. China
Get access

Abstract

Based on the microscopic observations and measurements, the mechanics behaviors of the nanostructured material (the surface-nanocrystallized Al-alloy material) at microscale are investigated experimentally and theoretically. In the experimental research, the hardness-indent depth curves or relations are measured by using both the method of randomly selecting loading points on the specimen surface and the continuous stiffness method. In the theoretical simulation, based on both the material microstructure characteristics and the experimental features of the nanoindentation, the microstructure cell model is developed and the strain gradient plasticity theory is adopted. The material hardness-indent depth curves are predicted and simulated. Through comparison of the experimental results with the simulation results, the material parameters and the model parameters are determined.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Valiev, RZ, Korznikov, AV, Mulyukov, RR. Mater. Sci. Eng., A168, 141(1993).Google Scholar
2. Valiev, RZ, Islamgaliev, RK, Alexandrov, IV. Prog. in Mater. Sci., 45, 103(2000).Google Scholar
3. Lu, K, Lu, J. J. Mater. Sci. & Tech., 15, 193(1999).Google Scholar
4. Fleck, NA, Hutchinson, JW. Adv. in Appl. Mech., 33, 295(1997).Google Scholar
5. Gao, H, Huang, Y, Nix, WD, Hutchinson, JW. J. Mech. Phys. Solids, 47, 1293(1999).Google Scholar
6. Wei, Y, Wang, X, Zhao, M, Cheng, CM, Bai, Y. Acta Mechanica Sinica, 19, 59(2003).Google Scholar
7. Wei, Y, Wang, X, Wu, X, Bai, Y. Science in China (Series A), 44, 74(2001).Google Scholar
8. Hill, R. J. Mech. Phys. Solids, 13, 89(1965).Google Scholar
9. Wei, Y, Hutchinson, JW. J. Mech. Phys. Solids, 45, 1253(1997).Google Scholar
10. Chen, JY, Wei, Y, Huang, Y, Hutchinson, JW, Hwang, KC. Eng. Fracture Mech., 64, 625(1999).Google Scholar