Strength of Coherently Strained Nanolayers Under HighTemperature Nanoindentation

Published online by Cambridge University Press:  26 February 2011

Mok Yew P'ng
Affiliation:
m.y.png@qmul.ac.uk, Queen Mary, University of London, Materials, Materials Department,, Queen Mary, University of London,, Mile End Road, London, E1 4NS, United Kingdom, 44 (0)2078823762
X. D. Hou
Affiliation:
x.hou@qmul.ac.uk, Queen Mary, University of London, Centre of Materials Research, Mile End Road, London, E1 4NS, United Kingdom
D. J. Dunstan
Affiliation:
D.Dunstan@qmul.ac.uk, Queen Mary, University of London, Centre of Materials Research, Mile End Road, London, E1 4NS, United Kingdom
A. J. Bushby
Affiliation:
A.J.Bushby@qmul.ac.uk, Queen Mary, University of London, Centre of Materials Research, Mile End Road, London, E1 4NS, United Kingdom
Get access

Abstract

Semiconductor strained layer superlattices are an ideal model material tostudy the effects of coherency strain in plasticity, due to the fine controlof nanolayer thickness and internal strain afforded by MBE deposition.Previously, nanoindentation of bulk InGaAs at 300K gave a yield pressure of6GPa (Jayawera et al Proc. Roy Soc, A459, 2049, 2003) while bending at 500centigrade gave a yield value of 30MPa (Pp’ ng et al Phil. Mag. 85, 4429,2005). In contrast, coherently strained InGaAs superlattices gavenanoindentation values of 3GPa at room temperature and bending at 500oC gavea yield value also around 3GPa. It appears that the coherency strain canimpart an athermal strengthening to the superlattice. It is clearlynecessary to do mechanical testing over the range 300-800K that will be ableto link the room temperature nanoindentation with the results from the hightemperature bending experiment and to determine the relationship betweenstrength, coherency strain and temperature. Preliminary experiments on thesesamples at elevated temperatures using a hot stage and the UMISnanoindentation system is difficult but feasible with the help of AFM toverify the contact area.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCE

1. Fischer-Cripps, A. C., Vacuum, 58, 569 (2000)Google Scholar
2. Bushby, A. J., Non-destructive testing and evaluation, 17, 213 (2001)Google Scholar
3. Fischer-Cripps, A. C., Nanoindentation, (Springer, 2004)Google Scholar
4. Pool, R., Science, 247, 643 (1990)Google Scholar
5. Jalili, N., Laxminarayana, K., Mechatronics, 14, 907 (2004)Google Scholar
6. P'ng, K. M. Y., Bushby, A. J., Dunstan, D. J., Philosophical Magazine, 85, 4429 (2005)Google Scholar
7. Jayaweera, N. B., Downes, J. R., Frogley, M. D., Hopkinson, M., Bushby, A. J., Kidd, P., Kelly, A., and Dunstan, D. J., Proc. Roy. Soc. A., 459, 2049 (2003)Google Scholar
8. Dunstan, D.J., J. Mat. Sci.: Materials in Electronics, 8, 337 (1997).Google Scholar
9. Madelung, O., Semiconductors Group IV Elements and III-V compounds, (Springer-Verlag, 1991)Google Scholar
10. Lim, Y. Y., Chaudhri, M. M., Philosophical Magazine, 84, 2877 (2004)Google Scholar
11. Hill, R., Storakers, B., Zdunek, A. B., Proc. Roy. Soc. A, 423, 301 (1989)10.1098/rspa.1989.0056Google Scholar
12. Saha, R., Nix, W.D., Materials Science and Engineering A, 319321, 898 (2001)Google Scholar
13. Lloyd, S. J., P'ng, K. M. Y., Clegg, W. J., Bushby, A. J., Dunstan, D. J., Philosophical Magazine, 85, 2469 (2005)Google Scholar
14. Yonenaga, I., Sumino, K., Phys. Stat. Sol. (a), 131, 663 (1992)Google Scholar
15. Schmidt, I., Gross, D., Proc. Roy Soc. Lond. A., 455, 3085 (1999)Google Scholar