Hostname: page-component-7857688df4-rx4j2 Total loading time: 0 Render date: 2025-11-14T01:10:18.412Z Has data issue: false hasContentIssue false

Strength of Single Crystal Al2O3 Fibers in Ni-Based Intermetallic and Superalloy Composites

Published online by Cambridge University Press:  15 February 2011

Randy R. Bowman
Affiliation:
NASA Lewis Research Center, 21000 Brookpark Road, Cleveland, Ohio 44135.
Ivan E. Locci
Affiliation:
NASA Lewis Research Center, 21000 Brookpark Road, Cleveland, Ohio 44135. Case Western Reserve University, Cleveland, Ohio 44106.
Susan L. Draper
Affiliation:
NASA Lewis Research Center, 21000 Brookpark Road, Cleveland, Ohio 44135.
Ajay K. Misra
Affiliation:
NYMA Inc., NASA-Lewis Group, BrookPark, Ohio 44142.
Get access

Abstract

Strength degradation of single crystal Al2O3 fibers due to the effect of fiber/matrix interaction and processing of NiAl and superalloy matrix composites, was investigated. Strength loss was quantified by tensile testing fibers that were exposed to the matrix alloy using two different methods. In one method, the fibers were incorporated into a composite by either the Powder Cloth (P-C) or binderless powder technique. The fibers were then extracted from the composite by chemical dissolution of the matrix and subsequently tensile tested and examined by scanning electron microscopy. In the other method, fibers were sputter-coated with a similar matrix composition and heat-treated to simulate conditions similar to those experienced during composite powder fabrication methods. In the sputter coating method, the contribution of fiber-matrix reaction on fiber strength loss was isolated from the effects of the various mechanical loads which are present during powder fabrication. For all matrices studied, significant strength loss was observed both in fibers extracted from composites and in fibers sputter-coated and annealed. Although surface ridges and pores were observed on the degraded fibers, it remains uncertain whether these features were responsible for the strength loss.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1994

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Calow, C. and Moore, A., J. Mat. Sci., 7, 543 (1972).Google Scholar
2. Pickens, J. W., Noebe, R. D., Watson, G. K., Brindley, P. K., Draper, S. L.: NASA Technical Memorandum 102060 (1989).Google Scholar
3. Draper, S. L. and Locci, I. E.: J. Mater. Res., 9, No. 6, June 1994.Google Scholar
4. Bowman, R. R., Misra, A. K., and Arnold, S. M., submitted to Metall. Trans., 1994.Google Scholar