Hostname: page-component-5b777bbd6c-pf7kn Total loading time: 0 Render date: 2025-06-24T18:30:23.674Z Has data issue: false hasContentIssue false

Surface Analysis Of The Nanocrystalline Fe-Based Alloys By Conversion Electron Mossbauer Spectroscopy

Published online by Cambridge University Press:  21 February 2011

A. Grabias
Affiliation:
Institute of Electronic Materials Technology, Wólczyńska 133, PL 01-919 Warsaw, Poland
M. Kopcewicz
Affiliation:
Institute of Electronic Materials Technology, Wólczyńska 133, PL 01-919 Warsaw, Poland
B. Idzikowski
Affiliation:
Institute of Molecular Physics, Polish Academy of Sciences, M. Smoluchowskiego 17, PL 60-179 Poznań, Poland
Get access

Abstract

A combined conversion electron and γ-transmission Mössbauer spectroscopy is applied to investigate the differences in the surface and bulk crystallization of the amorphous Fe-M-B-Cu (M: Zr, Ti, Nb, Ta) alloys. It is shown that the surface crystallization occurs at an annealing temperature lower than in the bulk. The nanocrystalline bcc Fe phase is significantly more abundant at the surface than in the bulk in the entire annealing temperature range.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Kopcewicz, M., Grabias, A., Idzikowski, B., J. Magn. Magn. Mat. 177–181, 1434 (1998).Google Scholar
2. Miglieríni, M., Kopcewicz, M., Idzikowski, B., Horváth, Z.E., Grabias, A., Škoránek, I., Dluzewski, P., Daróczi, Cs.S., J. Appl. Phys. 85, 1014 (1999).Google Scholar
3. Saegusa, N. and Morrish, A.H., Phys. Rev. B 26, 6547 (1982).Google Scholar
4. Zemčik, T., Závěta, K., Škorvánek, I., J. Mater. Sci. 28, 654 (1993).Google Scholar
5. Gonser, U., Ackermann, M., Wagner, H.G., J. Magn. Magn. Mat. 31–34, 1605 (1983).Google Scholar
6. Kopcewicz, M. and Grabias, A., J. Appl. Phys. 80, 3422 (1996).Google Scholar
7. Grabias, A. and Kopcewicz, M., Mater. Sci. Forum 269–272, 725 (1998).Google Scholar
8. Hesse, J. and Rübartsch, A., J. Phys. E 7, 526 (1974).Google Scholar
9. Caer, G. Le and Dubois, J.M., J. Phys. E 12, 1083 (1979).Google Scholar
10. Brand, R.A., Lauer, J., Herlach, D.M., J. Phys. F 13, 675 (1983).Google Scholar
11. Kopcewicz, M., Grabias, A., Nowicki, P., Proc. Rapidly Quenched and Metastable Materials RQ9 (Bratislava, Slovakia, 1996), Mater. Sci. Eng. A Suppl., Elsevier, (1997), p. 95.Google Scholar
12. Kopcewicz, M., Grabias, A., Williamson, D.L., J. Appl. Phys. 82, 1747 (1997).Google Scholar