Hostname: page-component-68c7f8b79f-xc2tv Total loading time: 0 Render date: 2025-12-23T20:03:34.736Z Has data issue: false hasContentIssue false

Thin Film Mechanical Properties Through Nano-Indentation

Published online by Cambridge University Press:  10 February 2011

Indira Adhihetty
Affiliation:
Technology Test and Analysis Lab., ATL, Motorola Inc. 2200 West Broadway, MD# M-360, Mesa, 85202
Jennifer Hay
Affiliation:
Applied Nano Metrics, Inc., P.O. Box 26,Stormville, NY 12582
Wei Chen
Affiliation:
Technology Test and Analysis Lab., ATL, Motorola Inc. 2200 West Broadway, MD# M-360, Mesa, 85202
Paddy Padmanabhan
Affiliation:
Technology Test and Analysis Lab., ATL, Motorola Inc. 2200 West Broadway, MD# M-360, Mesa, 85202
Get access

Abstract

Measuring material properties of sub-micron layers is an important yet a difficult task due to unavailability of proper instrumentation. Techniques such as Dynamic mechanical analysis has been used heavily in the last few years to measure modulus and glass transition temperature. But sample arrangement in this technique makes it impossible to use when thicknesses are smaller than 100 μm.After carefull study of number of different techniques availbale in different laboratories nanoindentation was selected as one of the most suitable, hence this technique can measure mechanical properties without removing the film from the substrate and also at various points of the film. This paper discusses the modulus measurement of thin poymeric films. A possible application of this technique as an adhesion tester will also be highlighted.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Oliver, W. C. and Pharr, G. M., J. Mater. Res. 7, 1564 (1992)Google Scholar
2. Pharr, G. M. and Oliver, W. C., MRS Bulletin XVII, 28 (1992)Google Scholar