Time-Dependent Deformation in Room-Temperature Indentation Experiments using a Nanoindenter

Published online by Cambridge University Press:  22 February 2011

Shefford P. Baker
Affiliation:
Stanford University, Department of Materials Science and Engineering, Stanford, CA 94305
Troy W. Barbee Jr
Affiliation:
Lawrence Livermore National Laboratory, Livermore, CA 94550
William D. Nix
Affiliation:
Stanford University, Department of Materials Science and Engineering, Stanford, CA 94305
Get access

Abstract

Time-dependent deformation in room-temperature indentation is a well known phenomenon which is frequently overlooked in depth-sensing indentation experiments. In this study, the time-dependent displacements which occur during depth-sensing indentation experiments using a Nanoindenter were investigated. Time-dependent displacements were found to result both from plastic deformation of the sample and experimental drift. A simple correction for experimental drift was applied in experiments on sputtered copper thin films and reasonable strain rate sensitivities were obtained. The sources of experimental drift were identified and measured. It appears to be possible to measure the rate-dependence of plastic deformation in a variety of materials using this instrument.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Doerner, M.F. and Nix, W.D., J. Mater. Res. 1, 601 (1986)CrossRefGoogle Scholar
2. Mayo, M.J. and Nix, W.D., Acta Metall. 6, 2183 (1988)Google Scholar
3. Hargreaves, F., J. Inst. Metals 39, 301 (1928)Google Scholar
4. Atkins, A.G., Silvério, A. and Tabor, D., J. Inst. Metals 94, 369 (1966)Google Scholar
5. Walker, W.W., in “The Science of Hardness Testing and its Research Applications” edited by Westbrook, J.H. and Conrad, H. (ASM, 1973)Google Scholar
6. Gunasekera, S.P. and Holloway, D.G., Phys. Chem. Glasses 14, 45 (1973)Google Scholar
7. Westbrook, J.H. and Jorgenson, P.J., Trans AIME 233, 425 (1965)Google Scholar
8. Carreker, R.P. Jr and Hibbard, W.R. Jr, Acta Metall. 1, 454 (1953)CrossRefGoogle Scholar