Hostname: page-component-68c7f8b79f-rgmxm Total loading time: 0 Render date: 2025-12-24T08:56:50.354Z Has data issue: false hasContentIssue false

Viscoelastic Analysis of Micro- and Nanoindentation

Published online by Cambridge University Press:  10 February 2011

Liangsheng Cheng
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, cheng6@msi.umn.edu
L. E. Scriven
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, cheng6@msi.umn.edu
William W. Gerberich
Affiliation:
Department of Chemical Engineering and Materials Science, University of Minnesota, Minneapolis, MN 55455, cheng6@msi.umn.edu
Get access

Abstract

The responses of viscoelastic solids indented by flat-ended cylindrical and spherical tip indenters are analyzed in this paper. The viscoelastic solid is a semi-infinite medium described by a standard three-element model. The theoretical relaxation and creep solutions are derived for a viscoelastic half-space using the method of functional equations. These solutions can apply to the responses of compressible as well as incompressible coatings to flat-ended cylindrical punch and spherical tip indentation. They establish a fundamental basis for probing mechanical properties of polymeric coatings with micro- and nanoindentation tests. To obtain the strain and stress distributions, an explicit finite difference method is employed to solve a viscoelastic indentation problem. The experimental creep and relaxation tests are conducted on both bulk polystyrene and polyurethane coatings. The viscoelastic properties are derived by fitting the theoretical solutions with the experimental data measured.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Lee, E.H. and Radok, J.R.M., “The contact problem for viscoelastic bodies”, J. Appl. Mech., 30, 438444 (1960).Google Scholar
2. Hunter, S.C., “The Hertz problem for a rigid spherical indenter and a viscoelastic halfspace”, J. Mech. Phys. Solids, 8, 219234 (1960).Google Scholar
3. Yang, W.H., “The contact problem for viscoelastic bodies”, J. AppI. Mech., 33, 395401 (1966).Google Scholar
4. Ting, T.C.T., “The contact stresses between a rigid indenter and a viscoelastic half-space”, J. Appl. Mech., 33, 845854 (1966).Google Scholar
5. Hunter, S.C., “The solution of boundary value problems in linear viscoelasticity”, In Proceedings of the fourth symposium on naval structural mechanics, Lafayette, Ind., Eringen, A. C., Liebowitz, H., Koh, S. L. and Crowley, J. M. (eds.), New York: Pergamon Press, 257295 (1967).Google Scholar
6. Findley, W.N., Lai, J.S. and Onaran, K., Creep and relaxation of nonlinear viscoelastic materials, with an introduction to linear viscoelasticity, New York: North-Holland Publishing Company, (1976).Google Scholar
7. Cheng, L.S., Numerical modeling of indentation and scratch problems, Ph. D. Dissertation, University of Minnesota, Minneapolis, (1996).Google Scholar
8. de Boer, M.P. and Gerberich, W.W., “Microwedge indentation of the thin film fine line-I. mechanics”, Acta Mater., 44, 31693175 (1996a).Google Scholar
9. de Boer, M.P. and Gerberich, W.W., “Microwedge indentation of the thin film fine line-II. experiment”, Acta Mater., 44, 31773187 (1996b).Google Scholar
10. Meares, P., Polymers: structure and bulk properties, New York: Van Nostrand, (1965).Google Scholar
11. Ferry, J.D., Viscoelastic properties of materials, 3rd ed., New York: Wiley, (1980).Google Scholar
12. Sperling, L.H., Introduction to physical polymer Science, New York: Wiley, (1986).Google Scholar
13. Lee, E.H., “Stress analysis in visco-elastic bodies”, Q. Appl. Math., 13, 183190 (1955).Google Scholar
14. Lee, E.H., “Viscoelastic Stress Analysis”, In Proceedings of the first symposium on naval structural mechanics, Stanford University, Goodier, J. N. and Hoff, N. J. (eds.), New York: Pergamon Press, 456482 (1960).Google Scholar
15. Lee, E.H., “Viscoelasticity”, In Handbook of engineering mechanics, 1st ed., Fluigge, W. (ed.), New York: McGraw-Hill, 53.153.22 (1962).Google Scholar
16. Radok, J.R.M., “Visco-elastic stress analysis”, Q. Appl. Math., 15, 198202 (1957).Google Scholar
17. Cheng, L.S., “Viscoelastic behavior in nanoindentation: model”, In Presentation in the coating process fundamentals program session of the center for interfacial engineering: Annual Review, University of Minnesota, Minneapolis, (1997).Google Scholar
18. Wilkins, M.L., “Fundamental methods in hydrodynamics”, Methods in Computational Physics, 3, New York: Academic Press, 211263 (1964).Google Scholar