Hostname: page-component-76fb5796d-22dnz Total loading time: 0 Render date: 2024-04-26T04:58:37.063Z Has data issue: false hasContentIssue false

A Comparison of the Behaviour of Vitrified HLW in Repositories in Salt, Clay and Granite. I: Experimental

Published online by Cambridge University Press:  21 February 2011

L. A. Mertens
Affiliation:
Hahn-Meitner-Institut, Glienicker Strasse 100, 1000 Berlin 39, FRG
W. Lutze
Affiliation:
Hahn-Meitner-Institut, Glienicker Strasse 100, 1000 Berlin 39, FRG
J. A. C. Marples
Affiliation:
AERE Harwell, Oxfordshire, OX11 ORA, UK
P. van Iseghem
Affiliation:
SCK/CEN, Boeretang 200, 2400 Mol, Belgium
E. Vernaz
Affiliation:
CEA Valrho, Marcoule BP 171, 30205 Bagnols sur Cèze, France
Get access

Extract

Laboratories from 11 countries participated in a ‘Round Robin’ comparative test excercise using the European Commission's Repository Systems Simulation Test [1,5]. The compulsory core part of this exercise involved testing an inactive simulant of the French high-level waste glass (SON68) in containers in which the conditions were similar to those that might occur after disposal of vitrified waste in a future repository. There were three options for the test, representing repositories in clay, granite and salt. Fifteen laboratories, mostly from within the European Community, but including laboratories from USA, Canada and Japan took part in the Round Robin. Most of the laboratories only covered one option: clay, 3, granite, 10, and salt 6. The test procedure was closely specified by the European Communities. This contribution and a companion paper [2] summarize the acquired information.

The HLW borosilicate glass SON68 (R7T7), to be returned to and eventually disposed of in various geological repositories by Cogema's reprocessing customers, was tested in a stainless steel autoclave developed and provided by CEA, Marcoule. The glass was prepared and delivered by CEA; together with crushed granite, sand, smectite and groundwater for the granite option. SCK-Mol provided the clay, smectite, sand and the recipe for claywater, HMI-Berlin the recipe for the rock salt composition. The analytical method was the only variable to be chosen by the participants. After termination of the experiments (duration 14-364d, temperature 90°C), the concentrations of the glass constituents Si, B, Mo, Li, in solution had to be determined. The data base was used to evaluate the test procedure and to identify analytical problems.

Type
Research Article
Copyright
Copyright © Materials Research Society 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Workshop on Testing of High-Level Waste Forms Under Repository Conditions, Cadarache France Oct. 17–21, 1988, Report EUR 12017 EN (1989).Google Scholar
[2] Marples, J. A. C. et al. this symposium.Google Scholar
[3] Henrion, P. et al., Radioactive Waste Management and the Nuclear Fuel Cycle, 3–4 (1985) pp. 313360 Google Scholar
[4] Heimann, R., Report AECL 9058 (1988).Google Scholar
[5] E.C. Repository Systems Simulation Test - Final Report, EUR 12544 EN (1989).Google Scholar