Corrosion of Carbon-Steel Containers for Heat-Generating Nuclear Waste in Brine Environments Relevant for A Rock-Salt Repository

Published online by Cambridge University Press:  25 February 2011

E. Smailos
Affiliation:
Kernforschungszentrum Karlsruhe GmbH, P.O. Box 3640, W-7500 Karlsruhe 1, GERMANY
W. Schwarzkopf
Affiliation:
Kernforschungszentrum Karlsruhe GmbH, P.O. Box 3640, W-7500 Karlsruhe 1, GERMANY
B. Kienzler
Affiliation:
Kernforschungszentrum Karlsruhe GmbH, P.O. Box 3640, W-7500 Karlsruhe 1, GERMANY
R. KÖster
Affiliation:
Kernforschungszentrum Karlsruhe GmbH, P.O. Box 3640, W-7500 Karlsruhe 1, GERMANY
Get access

Abstract

In previous corrosion studies, carbon steels, especially the fine-grained steel TStE355, were identified as promising materials for heat-generating nuclear waste containers acting as a barrier in a rock-salt repository. In the present study detailed investigations have been performed on fine-grained steel to determine the influence of important parameters on its corrosion behaviour in disposal-relevant salt brines. These parameters are: brine composition (Mg Cl2-rich and NaCI-rich brines), temperature (90°C, 170°C), and salt impurities, such as H2S concentrations of 25 mg/I-200 mg/I salt brine.

Under the conditions of the tests used here, carbon steel was subjected to general corrosion. Pitting and crevice corrosion or stress-corrosion cracking were not observed. The increase in temperature from 90°C to 170°C strongly enhanced the corrosion rate of the steel. In the MgCl2-rich brines, considerably higher rates (37-70 μm/a at 90°C, 200-300 °m/a at 170°C) were observed than in the NaCI-rich brine (5 μm/a at 90°C, 46 μm/a at 170°C). H2S concentrations in the MgCl2-rich Qbrine of up to 200 mg/l did not influence significantly the corrosion rate of the steel. The corrosion rates determined imply corrosion allowances that are technically acceptable for thick-walled containers. In view of these results, fine-grained steel continues to be considered as a promising material for long-lived HLW containers.

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Smailos, E., “Korrosionsuntersuchungen an ausgewahlten metallischen Werkstoffen als Behaltermaterialien fOr die Endlagerung von hochradioaktiven Abfallprodukten in Steinsalzformationen”, KfK Report No. 3953, 1985.Google Scholar
[2] Smailos, E., Schwarzkopf, W., Köster, R. and Grunthaler, K.H., “Advanced corrosion studies on selected packaging materials for disposal of HLW canisters in rock salt”, Proc. of the Symposium on Waste Management 1988 at Tucson, Arizona, February 28 - March 3, 1988.Google Scholar
[3] Köster, R., “Ausgewahlte Aspekte der Endlagerung radioaktiver Abfalle in Steinsalzformationen”, Schriftreihe der Universitat Regensburg, Band 13, S. 71-85, 1986.Google Scholar
[4] Smailos, E., Schwarzkopf, W., Köster, R. et al. , “Corrosion testing of selected packaging materials for disposal of high-level waste glass in rock-salt formations”, KfK Report No. 4723, 1990.Google Scholar
[5] Kienzler, B., Smailos, E., Köster, R., “Statistical evaluation and forecasting of steel corrosion data”, SAS European Users Group International (SEUGI 91) Symposium, June 11-14, 1991, Amsterdam.Google Scholar
[6] Westerman, R.E., Haberman, J.H. et al. , “Corrosion and environmentalmechanical characterisation of iron-base nuclear waste package structural barrier materials”, PNL Report No. 5426, 1986.CrossRefGoogle Scholar