Hostname: page-component-848d4c4894-wg55d Total loading time: 0 Render date: 2024-05-03T20:44:19.178Z Has data issue: false hasContentIssue false

Evaluation of four curing agents of epoxy resin and their effects above their thermal and dinamomechanical properties

Published online by Cambridge University Press:  13 July 2016

Aida E. García Valdez
Affiliation:
Centro de Investigación en Química Aplicada, Blvd Enrique Reyna Hermosillo #140, San José de los cerritos, C.P.25294, Saltillo Coahuila, México. (844)4-38-98-30
Ricardo Acosta Ortiz
Affiliation:
Centro de Investigación en Química Aplicada, Blvd Enrique Reyna Hermosillo #140, San José de los cerritos, C.P.25294, Saltillo Coahuila, México. (844)4-38-98-30
Lydia Berlanga Duarte
Affiliation:
Centro de Investigación en Química Aplicada, Blvd Enrique Reyna Hermosillo #140, San José de los cerritos, C.P.25294, Saltillo Coahuila, México. (844)4-38-98-30
Jorge Felix Espinosa
Affiliation:
Centro de Investigación en Química Aplicada, Blvd Enrique Reyna Hermosillo #140, San José de los cerritos, C.P.25294, Saltillo Coahuila, México. (844)4-38-98-30
Maria de L. Guillén Cisneros
Affiliation:
Centro de Investigación en Química Aplicada, Blvd Enrique Reyna Hermosillo #140, San José de los cerritos, C.P.25294, Saltillo Coahuila, México. (844)4-38-98-30
Get access

Abstract

Were synthesized four new hybrid hardener agents type amino tertiary functionalized with allyl groups from : l, 6-Hexanediamine, Diethylenetriamine, Trietilentriamine and Tris (2-aminoethyl) amine, using the basic nucleophilic substitution mechanism, replacing bromide by amino tertiary group in the presence of tetrabutylammonium bromide as phase transfer agent, producing allyl amine corresponding: ALA-4, ALA-5, ALA-6 and TRIS respectively, which were evaluated as a hardening of epoxy resin DGEBA through photopolymerization process by UV ligth curing, adding a 10, 20 and 40% molar percentage of hybrid materials and the thiol corresponding to carry out the thiol-ene reaction (TMP TMP, PTKMP) with DMPA as initiator. The resinic materials obtained, were evaluated by the technique of dynamic mechanical analysis (DMA) at a heating rate of 5° C/min in a range from - 50° C to 150° C in nitrogen atmosphere. The formulations with hybrid hardening agent ALA 4- 20% -PTKMP and TRIS 10% -PTKMP were the materials with modulus 2289, 2971 Mpa and tgs of 102,103°C, respectively.

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Decker, D., Moussa, K., Makromol. Chem. 191, 963 (1990).CrossRefGoogle Scholar
Decker, D., Moussa, K., EUR. Polymer J. 26, 393 (1990).CrossRefGoogle Scholar
Carioscia, J. A., Liu, H., Stansbury, J. W., Bowman, C. N., Polymer 48, 1526 (2007).CrossRefGoogle Scholar
Hoyle, C. E., Lee, T. Y., Roper, T. T., J. Polym. Sci: Part A: Polym. Chem. 42, 5301 (2004).CrossRefGoogle Scholar
Saln B, M. N. “Tecnología de proceso y transformación de materiales” Editorial UPC, 2005, cap.5.2 ,p. 128.Google Scholar