Hostname: page-component-7857688df4-q9hl9 Total loading time: 0 Render date: 2025-11-20T02:35:14.903Z Has data issue: false hasContentIssue false

Evidence of a Correlation Between the Transition Temperature for Ordering and the Activation Energy for Ordering Kinetics in Ni75Al25-xFex Superalloys

Published online by Cambridge University Press:  26 February 2011

R. Kozubski
Affiliation:
institute of Physics, Jagellonian University, Reymonta 4, 30–059 Krakow, Poland
J. Soltys
Affiliation:
institute of Physics, Jagellonian University, Reymonta 4, 30–059 Krakow, Poland
M.C. Cadeville
Affiliation:
Groupe d'Etude des Materiaux Ketalliques, I.P.C.M.S., 4, rue Blaise Pascal, 67070 Strasbourg Cedex, France
V. Pierron-Bohhes
Affiliation:
Groupe d'Etude des Materiaux Ketalliques, I.P.C.M.S., 4, rue Blaise Pascal, 67070 Strasbourg Cedex, France
Get access

Abstract

Kinetics of long-range ordering was studied in the alloys Ni75Al25-xFex by means of in situ resistometry. The alloys under consideration exhibit a dramatic decrease of the "order-disorder" transition temperature Ttr with increasing X. After the existing theoretical models, the activation energy of long-range ordering should depend on one hand on the energy of ordering - related to Ttr -, and on the other hand, on the current value of the LRO degree. The performed measurements yield an experimental evidence of the above relationships. In addition, a considerable effect of magnetic order on LRO kinetics has also been registered. The results are qualitatively discussed in terms of the model of LRO kinetics in L12 structure proposed by Schoijet and Girifalco.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1992

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Schoijet, M. and Girifalco, L.A., J. Phys. Chem. Solids a) 29, 497 (1968); b) 29, 911 (1968).CrossRefGoogle Scholar
2. Fontaine, D. de, J. Phys. Chem. Solids 34, 1285 (1973).CrossRefGoogle Scholar
3. Gschwend, K., Sato, H. and Kikuchi, R., J. Chem. Phys. 69, 5006 (1978).CrossRefGoogle Scholar
4. Bakker, H. in Diffusion in Crystalline Solids, edited by Murch, G.E. and Nowick, A.S. (Academic Press, Inc., Orlando, 1984), pp.213234.Google Scholar
5. Masahashi, N., Kawazoe, M., Takasugi, T. and Izumi, O., Z. Metallk. 78, 788 (1987).Google Scholar
6. Efthimiadis, K.G., Antonopoulos, J.G. and Tsoukalas, I.A., Solid State Commun. 70, 903 (1989).CrossRefGoogle Scholar
7. Kozubski, R., Soltys, J. and Cadeville, M.C., J.Phys.: Condens. Matter 2, 3451 (1990).Google Scholar
8. Kozubski, R. and Cadeville, M.C., J.Phys.F: Met.Phys. 18, 2569 (1988).CrossRefGoogle Scholar
9. Shindo, D., Kikuchi, M., Hirabayashi, M., Hanada, S. and Izumi, O., Trans. Japan Inst. Metals 29, 956 (1988).CrossRefGoogle Scholar