Hostname: page-component-76fb5796d-5g6vh Total loading time: 0 Render date: 2024-04-26T16:23:12.067Z Has data issue: false hasContentIssue false

In-Situ Optical Characterization of Titanium Nitride Thin Films for Applications in Microelectronics

Published online by Cambridge University Press:  10 February 2011

P. Patsalas
Affiliation:
Aristotle University of Thessaloniki, Department of Physics, Solid State Physics Section, GR-54006 Thessaloniki, Greece, ppats@skiathos.physics.auth.gr
S. Logothetidis
Affiliation:
Aristotle University of Thessaloniki, Department of Physics, Solid State Physics Section, GR-54006 Thessaloniki, Greece
C.A. Dimitriadis
Affiliation:
Aristotle University of Thessaloniki, Department of Physics, Solid State Physics Section, GR-54006 Thessaloniki, Greece
Get access

Abstract

Titanium Nitride (TiNx) thin films were deposited on Si(100) by reactive magnetron sputtering. The varied deposition conditions were the substrate temperature (Td) (27 - 650 °C) and the negative bias voltage (Vb) applied to the substrate (0 - 200 V) in order to produce TiNx films with various compositions and structural characteristics. The deposition process was monitored in-situ by Spectroscopic Ellipsometry in the spectral range 1.5–5.5 eV. Determination of the film composition was made through the measured screened plasma energy ωps while the electrical resistivity of TiNx was studied in terms of the unscreened plasma energy ωpu. ωpu was calculated by an optical model including a Drude term and Lorentz oscillator terms and their dependence on Td and Vb was studied. The ωpu was found to increase with Vb until a saturation value was obtained. The saturation value of ωpu depends on the Tdpu describes better the TiNx films, since it is directly correlated with their metallic character in terms of the electrical resistivity.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Wittmer, M. Studer, B. and Melchior, H. J. Appl. Phys. 52, 5722 (1981).10.1063/1.329512Google Scholar
[2] Hara, T. Yamanoue, A. Iio, H. Inoue, K. Washidzu, G. and Nakamura, S. Jpn. J. Appl. Phys. 30, 1447 (1991).10.1143/JJAP.30.1447Google Scholar
[3] Cheung, W. Seefeld, H. von, Nicolet, M. A., Ho, F. and Iles, P. J. Appl. Phys. 52, 4297 (1981).10.1063/1.329283Google Scholar
[4] Glass, R. C., Spellman, L. M., Tanaka, S. and Davis, R. F., J. Vac. Sci Technol. A10, 1625 (1992).10.1116/1.578033Google Scholar
[5] Chen, W.D., Bender, H. Vandervost, W. and Maes, H.E., Surf. Interface Anal 12, 151 (1988).10.1002/sia.740120216Google Scholar
[6] Vasile, M.J., Emerson, A.B., Baiocchi, F.A., J. Vac. Sci. Technol. A8, 99 (1990).10.1116/1.576995Google Scholar
[7] Logothetidis, S. Meletis, E. and Kourouklis, G. J. Mat. Res. 14, 436 (1999).10.1557/JMR.1999.0062Google Scholar
[8] Patsalas, P. Charitidis, C. Logothetidis, S. Dimitriadis, C.A., Valassiades, O. Appl. Phys. Lett. (submitted).Google Scholar
[9] Patsalas, P. Charitidis, C. Logothetidis, S. to be presented at E-MRS Spring Meeting, Symposium A, 1–4 June 1999, Strasbourg, France.Google Scholar
[10] Wooten, F.Optical Properties of Solids’, Academic Press, New York, 1972.Google Scholar
[11] Logothetidis, S. Meletis, E. Stergioudis, G. and Adjaottor, A. Thin Solid Films 338, 304 (1999).10.1016/S0040-6090(98)00975-4Google Scholar
[12] Pecz, B. Frangis, N. Logothetidis, S. Alexandrou, I. Barna, P.B., Stoemenos, J. Thin Solid Films 268, 57 (1995).10.1016/0040-6090(95)06692-6Google Scholar