The Mechanical Properties in the Vicinity of Grain Boundaries in Ultrafine-Grained and Polycrystalline Materials Studied by Nanoindentations

Published online by Cambridge University Press:  15 March 2011

E. Schweitzer
Affiliation:
Department of Materials Science & Engineering, University Erlangen-Nuremberg 91058 Erlangen, Martensstrasse 5, Germany
K. Durst
Affiliation:
Department of Materials Science & Engineering, University Erlangen-Nuremberg 91058 Erlangen, Martensstrasse 5, Germany
D. Amberger
Affiliation:
Department of Materials Science & Engineering, University Erlangen-Nuremberg 91058 Erlangen, Martensstrasse 5, Germany
M. Göken
Affiliation:
Department of Materials Science & Engineering, University Erlangen-Nuremberg 91058 Erlangen, Martensstrasse 5, Germany
Get access

Abstract

The strength of structural materials strongly depends on the structure and properties of grain boundaries. Interfaces usually act as barriers to dislocation motion and therefore strengthen materials with decreasing grain size, quantitatively described by the well-known Hall-Petch relation. However, interfaces in nanocrystalline materials are often covered with impurities or second phases, which may influence the mechanical properties. With nanoindentation testing it is now possible to probe the strength of interfaces like grain boundaries directly on a nanometer scale. Therefore this method was used to investigate the properties in the vicinity of grain boundaries in polycrystalline materials with conventional grain size and in ultrafine-grained metals prepared by equal channel angular pressing (ECAP), where no impurities are introduced during processing. Measurements on an austenitic steel clearly show a decreasing hardness close to the interface opposite to the general expected behavior of strengthening. In this case segregation effects strongly influence the mechanical properties near the boundaries. The nanoindentation investigations on ultrafine-grained Al and Cu show a strong strain rate sensitivity. Inelastic effects are also found between unloading-loading segments during indentations.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Westbrook, J. H. and Wood, D.L., Journal of the Institute of Metals 91, 174 (1962-1963)Google Scholar
2. Braunovic, M. in: The science of hardness testing and its research applications, ed. Westbrook, J.H. and Conrad, H., American Society for Metals, Ohio, p. 329 (1973)Google Scholar
3. Göken, M., Kempf, M., Bordenet, M. and Vehoff, H., Surface and Interface Analysis 27, 302 (1999)Google Scholar
4. Göken, M. and Kempf, M., Z. Metallkde. 92, 1061 (2001)Google Scholar
5. Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, 1564 (1992)Google Scholar
6. Schweitzer, E., Göken, M., Metallkde, Z.. in press (2004)Google Scholar
7. Höppel, H. W., Xu, C., Kautz, M., Barta-Schreiber, N., Langdon, T. G., Mughrabi, H., in: Nanomaterials by Severe Plastic Deformation, edited by Zehetbauer, M. and Valiev, R., (Wiley-VCH, Weinheim, 2004) pp 677683 Google Scholar
8. Schwaiger, R., Moser, B., Dao, M., Chollacoop, N., and Suresh, S., Acta Mater. 51, 5159 (2003)Google Scholar
9. Kumar, K. S., Swygenhoven, H. van and Suresh, S., Acta Mater. 51, 5743 (2003)Google Scholar
10. Höppel, H. W., May, J. and Göken, M., Adv. Eng. Mater. 6, 219 (2004)Google Scholar