Nanoindentation Hardness of Compositionally Modulated Ti/TiN Multilayered Films

Published online by Cambridge University Press:  10 February 2011

Eiji Kusano
Affiliation:
Kanazawa Institute of Technology, AMS R&D Center, Matsutou, Ishikawa, Japan.
Masaru Kitagawa
Affiliation:
Kanazawa Institute of Technology, AMS R&D Center, Matsutou, Ishikawa, Japan.
Hidehito Nanto
Affiliation:
Kanazawa Institute of Technology, AMS R&D Center, Matsutou, Ishikawa, Japan.
Akira Kinbara
Affiliation:
Kanazawa Institute of Technology, AMS R&D Center, Matsutou, Ishikawa, Japan.
Get access

Abstract

A detailed study of microhardness of multilayered films has been strongly needed to reveal effects of film layer structures and deposition conditions on the film hardness. A nanoindentation method is a useful method to investigate mechanical properties of thin films prepared on substrate materials. In this respect we have deposited a several types of Ti/TiN multilayered films and estimated their hardness by a nanoindentation method. The desired compositional modulation was obtained by changing the flow rate of N2 gas periodically using a computer system. The modulation period has been varied from 10 to 40nm by changing a flow rate control pattern. The total thickness of the film was about 500nm including the underlayer of the TiO2(50nm)/Ti(50nm) multilayer for all samples with different modulation period. Substrates used in the experiment were borosilicate glass and not heated during film deposition. The compositional distribution toward to the film depth orientation was estimated by Auger electron spectroscopy. The dynamic hardness of the films has been estimated by a nanoindenter as a function of the modulation period. It was found that there existed an optimum modulation period of 20nm to enhance the film hardness by multilayer structure.. The maximum value of microhardness obtained for the optimum modulation period was 29GPa, which was much larger than that of the monolithic TiN coating of 15GPa. The hardness measurement results show that the behavior for dynamic hardness was different from that for plastic deformation hardness obtained.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Helmersson, U., Todorova, S., Barnett, S. A., Sundgren, J.-E.. Markett, L. C., and Greene, J. E., J.Appl.Phys. 62, 481(1987).Google Scholar
2.Shinn, M., Hultman, L., and Barnett, S. A., J.Mater.Res. 7, 901(1992).Google Scholar
3.Chu, X., Barnett, S. A., Wong, M. S., and Sproul, W. D., Surf. Coat.Technol. 57, 13(1993).Google Scholar
4.Ding, Y., Farhat, Z., Northwood, D. O., and Alpas, A. T., Surf. CoatTechnol. 68/69, 459(1994).Google Scholar
5.Hurkmans, T., Trinh, T., Lewis, D. B., Brooks, J. S., and Munz, W.-D., Surf CoatTechnol. 76/77, 159(1995).Google Scholar
6.Farhat, Z., Ding, Y., Northwood, D. O., and Alpas, A. T., Surf. Coat.Technol. 89, 24(1997).Google Scholar
7.Larsson, M., Bromark, M., Hedenqvist, P., and Hogmark, S., Surf. Coat.Technol. 76/77, 202(1995).Google Scholar
8.Ma, K. J., Bloyce, A., and Bell, T., Surf. Coat.Technol. 76/77, 297(1995).Google Scholar
9.Sproul, W. D., J.Vac.Sci.Technol.A12. 1595(1994).Google Scholar
10.Koehler, J. S., Phys.Review B2, 547(1970).Google Scholar
11.Holleck, H. and Schier, V., Surf. CoatTechnol. 76/77, 328(1995).Google Scholar
12.Weimer, A. W. in Carbide, Nitride, and Boride Materials Synthesis and Processing, edited by Weimer, A. W.(Chapman & Hall, London, 1997), p.650.Google Scholar