Nondestructive defect measurement and surface analysis of 3C-SiC on Si (001) by electron channeling contrast imaging

Published online by Cambridge University Press:  01 February 2011

Yoosuf N. Picard
Affiliation:
yoosuf.picard@nrl.navy.mil, Naval Research Lab, Electronics Science and Technology, Code 6812, 4555 Overlook Ave. SW, Washington, DC, 20375, United States
Christopher Locke
Affiliation:
clocke@helios.acomp.usf.edu, University of South Florida, Electrical Engineering Dept., 4202 E. Fowler Ave., Tampa, FL, 33620, United States
Christopher L. Frewin
Affiliation:
clfrewin@eng.usf.edu, University of South Florida, Electrical Engineering Dept., 4202 E. Fowler Ave., Tampa, FL, 33620, United States
Rachael L. Myers-Ward
Affiliation:
rachael.myers-ward@nrl.navy.mil, Naval Research Lab, Electronics Science and Technology, Code 6812, 4555 Overlook Ave. SW, Washington, DC, 20375, United States
Joshua D. Caldwell
Affiliation:
jcaldwel@ccs.nrl.navy.mil, Naval Research Lab, Electronics Science and Technology, Code 6812, 4555 Overlook Ave. SW, Washington, DC, 20375, United States
Karl D. Hobart
Affiliation:
karl.hobart@nrl.navy.mil, Naval Research Lab, Electronics Science and Technology, Code 6812, 4555 Overlook Ave. SW, Washington, DC, 20375, United States
Mark E. Twigg
Affiliation:
mark.twigg@nrl.navy.mil, Naval Research Lab, Electronics Science and Technology, Code 6812, 4555 Overlook Ave. SW, Washington, DC, 20375, United States
Stephen E. Saddow
Affiliation:
saddow@eng.usf.edu, University of South Florida, Electrical Engineering Dept., 4202 E. Fowler Ave., Tampa, FL, 33620, United States
Get access

Abstract

The electron channeling contrast imaging (ECCI) technique was utilized to investigate atomic step morphologies and dislocation densities in 3C-SiC films grown by chemical vapor deposition (CVD) on Si (001) substrates. ECCI in this study was performed inside a commercial scanning electron microscope using an electron backscatter diffraction (EBSD) system equipped with forescatter diode detectors. This approach allowed simultaneous imaging of atomic steps, verified by atomic force microscopy, and dislocations at the film surface. EBSD analysis verified the orientation and monocrystalline quality of the 3C-SiC films. Dislocation densities in 3C-SiC films were measured locally using ECCI, with qualitative verification by x-ray diffraction. Differences in the dislocation density across a 50 mm diameter 3C-SiC film could be attributed to subtle variations during the carbonization process across the substrate surface.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Trager-Cowan, C., Sweeney, E. Trimby, P.W. Day, A.P. Gholinia, A. Schmidt, N.H., Parbrook, P.J. Wilkinson, A.J. and Watson, I.M. Phys. Rev. B. 75, 085301 (2007).Google Scholar
2. Picard, Y.N. Caldwell, J.D. Twigg, M.E. Eddy, C.R. Jr., Mastro, M.A. Henry, R.L. Holm, R.T. Neudeck, P.G. Trunek, A.J. Powell, J.A. Appl. Phys. Lett. 91, 094106 (2007).Google Scholar
3. Picard, Y.N. Twigg, M.E. Caldwell, J.D. Eddy, C.R. Jr., Neudeck, P.G. Trunek, A.J. and Powell, J.A. Appl. Phys. Lett. 90, 234101 (2007).Google Scholar
4. Reyes, M. Shishkin, Y. Harvey, S. and Saddow, S. E. Mater. Sci. For. 556-557, 191 (2007).Google Scholar
5. Neudeck, P.G. Trunek, A.J. and Powell, J.A. Mater. Res. Soc. Symp. Proc. 815, J5.32.1 (2004).Google Scholar
6. Stevens, R. J. Mater. Sci. 5, 474 (1970).Google Scholar
7. Ning, X.J. and Pirouz, P. J. Mater. Res. 11, 884 (1996).Google Scholar
8. Coletti, C. Frewin, C.L. Saddow, S.E. Hetzel, M. Virojanadara, C. and Starke, U. Appl. Phys. Lett. 91, 061914 (2007).Google Scholar
9. Speer, K.M. Neudeck, P.G. Crimp, M.A. Burda, C. and Pirouz, P. Phys. Stat. Sol. A. 7, 2216 (2007).Google Scholar