Hostname: page-component-7f64f4797f-p4db6 Total loading time: 0 Render date: 2025-11-07T02:44:50.469Z Has data issue: false hasContentIssue false

On the Measurement of Creep by Nanoindentation with Continuous Stiffness Techniques

Published online by Cambridge University Press:  01 February 2011

Andrei Rar
Affiliation:
Oak Ridge National Laboratory, Metals and Ceramics Division, Oak Ridge, TN 37831, U.S.A. The University of Tennessee, Department of Materials Science and Engineering, Knoxville, TN 37996, U.S.A.
Sangjoon Sohn
Affiliation:
The University of Tennessee, Department of Materials Science and Engineering, Knoxville, TN 37996, U.S.A.
Warren C. Oliver
Affiliation:
MTS, Nano Instruments Innovation Center, Oak Ridge, TN 37831, U.S.A.
David L. Goldsby
Affiliation:
Department of Geological Sciences, Brown University, Providence, RI 02912, U.S.A.
Terry E. Tullis
Affiliation:
Department of Geological Sciences, Brown University, Providence, RI 02912, U.S.A.
George M. Pharr
Affiliation:
Oak Ridge National Laboratory, Metals and Ceramics Division, Oak Ridge, TN 37831, U.S.A. The University of Tennessee, Department of Materials Science and Engineering, Knoxville, TN 37996, U.S.A.
Get access

Abstract

Measurement of material creep parameters by means of nanoindentation using continuous stiffness techniques avoids the problems associated with thermal drift that often plague creep measurements based on the time dependence of the indentation depth alone [1, 2]. Problems with thermal drift are negligible from a practical point of view during continuous stiffness measurements because the contact stiffness can be measured over a short time period, typically less than one second, during which time the displacements due to thermal drift are minimal. Determination of the time dependence of the indentation depth from the stiffness data relies on the well-known relation between contact stiffness and the square root of the contact area. For pyramidal indenters, the true indentation contact depth must be proportional to the contact stiffness, leading to the assumption that indentation depth is also proportional to the contact stiffness. In this study, we critically examine this assumption using data obtained from experiments on a relatively soft material, epoxy, and a relatively hard material, fused quartz. The results show that just after initial load application, the change in contact area may be different than that expected from the change in indentation depth. One possible explanation for the observed behavior is examined by finite element modeling.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 2005

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Weihs, T. P. and Pethica, J.B‥, Mat. Res. Soc. Symp. Proc. 246, 325 (1992).Google Scholar
2. Goldsby, D. L., Rar, A., Pharr, G.M., and Tullis, T. E, J. Mater. Res. 18, 357 (2004).Google Scholar
3. Mayo, M.J. and Nix, W.D., Acta Metall. 36, 2183 (1988).Google Scholar
4. Lucas, B.N. & Oliver, W.C., Metall. Mater. Trans. A30, 601 (1999)Google Scholar
5. Cheng, Y. T. and Cheng, C. M., Philosophical Magazine Letters, Vol. 81, p.10 (2001)Google Scholar
6. Bower, A.F., Fleck, N.A., Needleman, A., and Ogbonna, N., Proc. R. Soc. Lond. A 441, 97 (1993).Google Scholar
7. Sneddon, I.N., Int. J. Eng. Sci. 3, 47 (1965).Google Scholar