Hostname: page-component-cb9f654ff-5jtmz Total loading time: 0 Render date: 2025-08-31T02:43:50.713Z Has data issue: false hasContentIssue false

A Phenomenological Approach to Simulating the Evolution of Radioactive-Waste Container Damage Due to Pitting Corrosion

Published online by Cambridge University Press:  15 February 2011

G. A. Henshall*
Affiliation:
Lawrence Livermore National Laboratory, L-355, Livermore, CA 94551.
Get access

Abstract

The damage to high-level radioactive-waste containers by pitting corrosion is an important design and performance assessment consideration. It is desirable to calculate the evolution of the pit depth distribution, not just the time required for initial penetration of the containers, so that the area available for release of radionuclides through the container can be estimated. A phenomenological approach for computing the time evolution of these distributions is presented which combines elements of the deterministic and stochastic aspects of pit growth. The consistency of this approach with the mechanisms believed to control the evolution of the pit depth distribution is discussed. Qualitative comparisons of preliminary model predictions with a variety of experimental data from the literature are shown to be generally favorable. The sensitivity of the simulated distributions to changes in the input parameters is discussed. Finally, the results of the current model are compared to those of existing approaches based on extremevalue statistics, particularly regarding the extrapolation of laboratory data to large exposed surface areas.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Shoesmith, D., ”Modelling to Predict the Corrosion Behavior of Nuclear Waste Containers,” presented at the Forum for the Use of Nickel Alloys for Radwaste Containers, Tucson, AZ, Feb. 2223 (1995).Google Scholar
2. Andrews, R. W., ”TSPA-95 Objectives and Approach: Focus on Waste Packages/EBS Conceptual Models,” presented at the NWTRB Full Board Meeting, Las Vegas, NV, Apr. 19–20, (1995).Google Scholar
3. Henshall, G. A., ”Modeling Pitting Corrosion Damage of High-Level Nuclear-Waste Containers using a Stochastic Approach,” J. Nucl. Mater. 195, 109 (1992).Google Scholar
4. Marsh, G. P., Bland, I. D., and Taylor, K. J., ”Statistical Study of Pit Propagation in Carbon Steel Under Nuclear Waste Disposal Conditions,” Br. Corros. J. 23, 157164 (1988).Google Scholar
5. Flaks, V. Y., ”Statistical Model of Size Distribution of Pittings During Atmospheric Corrosion of Aluminum Alloys,” Protection of Metals 9, 407409 (1973).Google Scholar
6. Provan, J. W. and Rodriguez, E. S., ”Part I: Development of a Markov Description of Pitting Corrosion,” Corros. 45, 178192 (1989).Google Scholar
7. Aziz, P. M., ”Application of the Statistical Theory of Extreme Values to the Analysis of Maximum Pit Depth Data for Aluminum,” Corros. 12, 495506 (1956).Google Scholar
8. Hoch, A., et al., “A Modelling and Experimental Study for Long-Term Prediction of Localised Corrosion in Carbon Steel Overpacks for High-Level Radioactive Waste,” in MRS Symposium on the Scientific Basis for Nuclear Waste Management XVIII, pp. 703–710 (1995).Google Scholar
9. Strutt, J. E., Nicholls, J. R., and Barbier, B., ”The Prediction of Corrosion by Statistical Analysis of Corrosion Profilesrdquo; Corros. Sci. 25, 305315 (1985).Google Scholar
10. Finley, H. F., ”An Extreme-Value Statistical Analysis of Maximum Pit Depths and Time to First Perforation,” Corros. 23, 8387 (1967).Google Scholar