Pt-CdS/TiO2 nanotube catalyst for photocatalytic reduction of CO2 with water under visible light irradiation

Published online by Cambridge University Press:  02 August 2011

Jian Yuan
Affiliation:
Research Center for Combustion and Environmental Technology, Shanghai Jiao Tong University, Shanghai 200240, P.R. China.
Chuanzhao Zhang
Affiliation:
Research Center for Combustion and Environmental Technology, Shanghai Jiao Tong University, Shanghai 200240, P.R. China.
Caolong Li
Affiliation:
Research Center for Combustion and Environmental Technology, Shanghai Jiao Tong University, Shanghai 200240, P.R. China.
Mingxia Chen
Affiliation:
Research Center for Combustion and Environmental Technology, Shanghai Jiao Tong University, Shanghai 200240, P.R. China.
Wenfeng Shangguan
Affiliation:
Research Center for Combustion and Environmental Technology, Shanghai Jiao Tong University, Shanghai 200240, P.R. China.
Get access

Abstract

Titanate nanotube (TNT) was prepared by alkaline hydrothermal method starting from TiO2 (P25), and then CdS-TNT was prepared for visible light harvesting by immersing TNT in Cd(CH3COO)2 and then (NH2)2CS aqueous solutions subsequently and heat treated at specialtemperature. After loading with Pt, photocatalytic reduction of gas phase CO2 with water vapor was carried out under UV-VIS and visible light irradiation. The results showed that the main reaction products were CH4, C2H4, C2H6 and H2, which were online characterized by gaschromatography when the flow rate of 5000 ppm CO2 is 0.35 ml/min. The hydrogenation process also realized under visible light illumination for Pt-CdS/TNT and producted 0.44 μmol/min CH4. The maximum yield of methane reached about 130 μmol/min when Pt-CdS/TNTwas irradiated with UV-Vis light. The time profile for production yield increased steadily with time up to about 6–7 h, then a decrease of the reaction rate occurred. It is suggested that thadsorption of intermediate products CO, O2 etc. on Pt and the oxidation of Pt might be the reasons for the photocatalytic reaction deterioration.

Type
Research Article
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Yamashita, H., Fuji, Y., Ichihashi, Y., Zhang, S.G., Ikeue, K., Park, D.R., Koyano, K., Tatsumi, T., Anpo, M., Catal Today. 45 (1998) 221 10.1016/S0920-5861(98)00219-3Google Scholar
2. Tseng, I.H., Chang, W.C., Wu, J.C.S., Appl Catal B: Environm. 37 (2002) 37 10.1016/S0926-3373(01)00322-8Google Scholar
3. Pan, P.W., Chen, Y.W.. Catalysis Communications. 8 (2007) 1546 10.1016/j.catcom.2007.01.006Google Scholar
4. Zhao, Z.H., Fan, J.M., Wang, Z.Z., Journal of Cleaner Production.15 (2007)1894 10.1016/j.jclepro.2006.05.003Google Scholar
5. Yu, K.P., Yu, W.Y., Kuo, M.Ch., Lion, Y.Ch., Chien, S.H., Applied Catalysis B: Enviromental. 84 (2008)112 10.1016/j.apcatb.2008.03.009Google Scholar
6. Varghese, O.K., Paulose, M., LaTempa, T. J.,Grimes, C. A.; Nano Lett. 9(2) (2009) 731 10.1021/nl803258pGoogle Scholar
7. Shangguana, W.F., Yoshida, A.. Solar Energy Materials & Solar Cells. 69 (2001) 189.10.1016/S0927-0248(01)00020-4Google Scholar
8. Hoyer, P., Langmuir, 12(1996)1411 10.1021/la9507803Google Scholar
9..Lakshimi, B B, Patrissi, C J, Martin, C R, Chem. Mater. 9 (1997) 2544 10.1021/cm970268yGoogle Scholar
10. Tan, S. S., Zou, L., Hu, E.; Catalysis Today 115 (2006) 269 10.1016/j.cattod.2006.02.057Google Scholar